Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.45 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.45 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene EX3-80 is a high density polyethylene with 1-Butene as co monomer. It is natural, good ESCR, good impact strength, tough and rigid pipe resin. Applications: pipe extrusion PE 80 class, industrial a.. |
|||
Melt Flow | 0.45 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.45 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX3 HM 5010 T2N High Density Polyethylene EX3 (HM 5010 T2N) is a natural colored high density polyethylene with Butene-1 as comonomer. The product is classified as PE 80 and good stress crack resistance properties combined with good impact .. |
|||
Melt Flow | 0.45 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.45 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® BB 75 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.45 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.45 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® FB 75 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.45 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® PL 10 HDPE Pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.45 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® VL 10 HDPE Extrusion and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.45 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE HD 7845.30 High Density Polyethylene Resin Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc.. |
|||
Melt Flow | 0.45 g/10 min @Load 5.00 kg |
0.45 g/10 min @Load 11.0 lb |
ISO 1133 |
Total Lacqtene® 2001 TBK 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TBK 46 is a high density polyethylene produced by the gas phase polymerization process. LACQTENE® 2001 TBK 46 is a black compound especially developed for pressure pipe for gas and .. |
|||
Melt Flow | 0.45 g/10 min @Load 5.00 kg |
0.45 g/10 min @Load 11.0 lb |
ISO 1133 |
Total Lacqtene® 2001 TN 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TN 46 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2001 TN 46 is used for sewage pipe, smooth protective condu.. |