Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gwent Electronic Materials C2050106D7 Carbon Graphite Ink

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2050106D7 Carbon Graphite Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This Carbon Graphite Ink is designed to be used for screen printing working electrodes. This is an ink which has been optimized to give superior electrochemical performance. It gives excellent electrochemical performance with good print properties and fine lines.Applications in Medical Diagnostics, DNA Sensors, Lab-on-a-Chip & Environmental SensorsScreen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156-230tpiSubstrate: polyester, PVC, polycarbonate or ceramicInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 38 - 41 %

@Temperature 130 °C
38 - 41 %

@Temperature 266 °F
Viscosity 12000 - 15000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
12000 - 15000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 15.5 microns
0.610 mil
Cured, Printed through 230 stainless steel mesh with 13 micron emulsion
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Surface Resistivity per Square 28.37 ohm

@Thickness 0.0250 mm
28.37 ohm

@Thickness 0.000984 in
Normalized, Printed through 230 stainless steel mesh with 13 micron emulsion
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 80.0 °C
0.167 hour

@Temperature 176 °F
30.0 min

@Temperature 60.0 °C
0.500 hour

@Temperature 140 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 250
Using a 230 mesh stainless steel screen