Thermal Properties Metric English Comments
Vicat Softening Point 67.0 °C
153 °F
ASTM D1525
DSM Biomedical CarboSil® 40 90A Biocompatible Silicone Polycarbonate Urethane  (discontinued **)
Combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic urethane elastomers. Noncytotoxic and nonhemolytic. Low-En..
Vicat Softening Point 67.0 °C
153 °F
Rate A; ISO 306/A50
Premix Thermoplastics PRE-ELEC® CP 1318  (discontinued **)
PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit..
Vicat Softening Point 67.0 °C

@Load 1.00 kg
153 °F

@Load 2.20 lb
ISO 306/A
Polimeri Europa Greenflex® FD 50 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 50 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FD 50 exhibit good optical and sealing properties, high flexibility and toughnes..
Vicat Softening Point 67.0 °C

@Load 1.00 kg
153 °F

@Load 2.20 lb
ISO 306/A
Polimeri Europa Greenflex® FD 53 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 53 is an ethylene vinyl acetate copolymer (EVA), containing antiblocking agent, for blown film extrusion. Films produced with Greenflex FD 53 exhibit good sealing properties, high flex..
Vicat Softening Point 67.0 °C
153 °F
Dow Pellethane® 2351-85AE Polyurethane Elastomer, Ether Based  (discontinued **)
PELLETHANE® 2351-85AE elastomer is a polyether hybrid specialty polyurethane elastomer compound which combines excellent resistance to fuels and oils with good hydrolytic stability and high damping..
Vicat Softening Point 67.0 °C
153 °F
ASTM D1525
Eastman 812A Polyethylene  (discontinued **)
Polyethylene 812A is a natural low density material with a 200 melt index. This high-flow formulation is used for specialty injection molding applications in the medical market.Unless otherwise not..
Vicat Softening Point 67.0 °C
153 °F
ASTM D1525
Eastman 812P Polyethylene  (discontinued **)
Polyethylene 812A is a natural low density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a carpet backing to bind fibers to the carpet...
Vicat Softening Point 67.0 °C
153 °F
ISO 306
Iran Petrochemical (PCC) EX3 HM 5010 T2N High Density Polyethylene
EX3 (HM 5010 T2N) is a natural colored high density polyethylene with Butene-1 as comonomer. The product is classified as PE 80 and good stress crack resistance properties combined with good impact ..
Vicat Softening Point 67.0 °C
153 °F
ASTM D1525
Lubrizol Estane® T365A Thermoplastic Polyurethane
Type: Estane® T365A is a Shore 70A, polyether grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor..
Vicat Softening Point 67.0 °C
153 °F
ASTM D1525
DuPont Elvax® 3165SB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Vicat Softening Point 67.0 °C
153 °F
ASTM D1525
DuPont Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Vicat Softening Point 67.0 °C
153 °F
D1525
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ EF529 is an ethylene vinyl acetate copolymer with 18.5% VA. It contains no slip or antiblock and is designed for blown and cast films requiring excellent optics and low heat seal ..
Vicat Softening Point 67.0 °C
153 °F
ASTM D1525
DSM Biomedical PurSil® 35 Thermoplastic Silicone Polyether Polyurethane (TSPU)
A novel copolymer that is strong yet flexible with proven biocompatibility and biostability Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional..
Vicat Softening Point 67.0 °C
153 °F
ASTM D1525, ISO 306
DuPont™ Bynel® 30E783 Anhydride Modified Ethylene Vinyl Acetate
BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Vicat Softening Point 67.0 °C
153 °F
50°C/hr; 50N
Arkema Group Rilsan® MB 3750 Nylon 11, Transparent Grade (Dry)
Designation ISO 1874-PA11/xx,F,THL,22-020Transparent semi-crystalline PA11 grade.Used for film extrusion and injection molding (low thickness).Very good low temperature impact strength.High chemical..
Vicat Softening Point 67.0 °C
153 °F
ASTM D1525
C.O.I.M. LARIPUR® LPR6515 Plasticized Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Vicat Softening Point 67.0 - 132 °C
153 - 270 °F
Average value: 120 °C Grade Count:54
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
Vicat Softening Point 67.0 °C
153 °F
A50; DIN 53460
Lubrizol ESTANE® 58214 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Vicat Softening Point 67.0 - 82.0 °C
153 - 180 °F
Average value: 74.0 °C Grade Count:3
Overview of materials for Silicone Polyurethane, Ether Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value..
Vicat Softening Point 67.0 °C
153 °F
ASTM D1525, ISO 306
DuPont Elvax® 3165Z Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 3165Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additives..
Vicat Softening Point 67.0 °C
153 °F
ASTM D1525, ISO 306
DuPont Elvax® 3172Z Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 3172Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additives..
Vicat Softening Point >= 67.0 °C
>= 153 °F
ASTM D 1525
Karina E 843-18/302-CRM Gray PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Vicat Softening Point 67.0 - 156 °C
153 - 313 °F
Average value: 137 °C Grade Count:11
Overview of materials for Polypropylene, Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values..
Vicat Softening Point >= 67.0 °C
>= 153 °F
ASTM D 1525
Karina E 843-18/302-CRM Gray PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.