Polymer Property : Melt Flow = 12 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 220 °C
12 g/10 min

@Load 11.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® MG94 ABS (Asia Pacific)
Superior flow, injection molding ABS. Good impact. For thin-wall applications.
Melt Flow 12 g/10 min

@Load 3.80 kg,
Temperature 230 °C
12 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Network Polymers NPP 808 C2WW
Description: Polycarbonate AlloyInformation provided by Network Polymers Inc.
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 260 °C
12 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Cycoloy® C4220K PC+ABS (Asia Pacific)
Cycoloy* C4220K resin is an injection moldable 20% glass reinforced non FR PC-ABS. Key features include improved Knit Line strength, good flow, excellent strength & rigidity, heat resistance & hyd..
Melt Flow 12 g/10 min

@Load 3.80 kg,
Temperature 200 °C
12 g/10 min

@Load 8.38 lb,
Temperature 392 °F
ASTM D 1238
SABIC Innovative Plastics Geloy XTWE280 ASA
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Americas region.
Melt Flow 12 g/10 min

@Load 3.80 kg,
Temperature 200 °C
12 g/10 min

@Load 8.38 lb,
Temperature 392 °F
ASTM D 1238
SABIC Innovative Plastics Geloy XTWE280 ASA (Europe-Africa-Middle East)
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 12 g/10 min

@Load 10.0 kg,
Temperature 220 °C
12 g/10 min

@Load 22.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Geloy XTWM200 ASA
ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 12 - 30 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 - 30 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio 30-50; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 4142L (424F5) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 12 g/10 min

@Load 1.20 kg,
Temperature 300 °C
12 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® I2220 PC
General purpose polycarbonate with melt flow rate of 10.5.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 12 g/10 min

@Load 1.20 kg,
Temperature 250 °C
12 g/10 min

@Load 2.65 lb,
Temperature 482 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® ML1010 PC (Europe-Africa-Middle East)
Superior performance, improved flow over standard grades at lower temperatures. Internal mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 190 °C
12 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Eraclene® MM 74 High Density Polyethylene - Injection Molding
Eraclene MM 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 74 is characterized by a good balance between rigidity and impact..
Melt Flow 12 g/10 min

@Load 1.20 kg,
Temperature 300 °C
12 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific)
DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r..
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 200 °C
12 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238(G)
LG Chemical ALPHALAC SF510 HIPS
Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa..
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 250 °C
12 g/10 min

@Load 11.0 lb,
Temperature 482 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC
Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im..
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 265 °C
12 g/10 min

@Load 4.76 lb,
Temperature 509 °F
ASTM D 1238
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Asia Pacific)
Mold Release version of X7200This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 265 °C
12 g/10 min

@Load 4.76 lb,
Temperature 509 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Asia Pacific)
Mold Release version of X7200This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 265 °C
12 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Techmer ES Plastiblend® PC/PBT IM 1012
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc.
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 260 °C
12 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Styrolution Novodur® 4115 ABS
Novodur Ultra 4115 is a PC modified high heat injection molding grade. It provides good heat resistance combined with high impact strength.Information provided by Styrolution
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 200 °C
12 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Styrolution Styrolux 3G33 SBC
Styrolux 3G33 is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion and thermoforming. It offers an outstanding combination of crystal clarity and ..
Melt Flow 12 g/10 min

@Load 3.80 kg,
Temperature 230 °C
12 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ISO 1133
Styron EMERGEâ„¢ 7500 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ PC/ABS 7500 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the..
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 265 °C
12 g/10 min

@Load 4.76 lb,
Temperature 509 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Xylex X7509UV PC+POLYESTER (Europe-Africa-Middle East)
PC+POLYESTER, Transparent, UV-Stabilized,This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 265 °C
12 g/10 min

@Load 4.76 lb,
Temperature 509 °F
ASTM D 1238
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis ME266U Polypropylene Compound, Mineral Filled
ME266U is a 20% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gives a good surface quality. ..
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis ME212U Polypropylene Compound, Mineral Filled
ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air..
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Delrin® 500AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring ..
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
Melt Flow 12 g/10 min

@Load 3.80 kg,
Temperature 230 °C
12 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Diamond Polymers NPP 60-908 Polyester Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 12 g/10 min

@Load 3.80 kg,
Temperature 230 °C
12 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Diamond Polymers NPP 808 C2 Polycarbonate Alloy, Natural
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 280 °C
12 g/10 min

@Load 11.0 lb,
Temperature 536 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Asia Pacific)
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..