Material Notes:
This is a homopolymer designed for tenter frame BOPP processing and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsFood packagingOverwrapMetallized filmBenefitsBarefootGood optical propertiesHigh strength propertiesInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Density 0.904 - 0.908 g/cc
0.0327 - 0.0328 lb/in³
ASTM D1505
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Melt Flow 3.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79 - 108
79 - 108
ASTM D785
Tensile Strength, Yield 31.6 MPa

@Temperature 23.0 °C
4580 psi

@Temperature 73.4 °F
Molded and tested under D410, 50 mm/min; ASTM D638
Elongation at Yield 10 %
10 %
50 mm/min; ASTM D638
Flexural Modulus 1.30 GPa

@Temperature 23.0 °C
188 ksi

@Temperature 73.4 °F
ASTM D790A
Izod Impact, Notched 0.214 - 0.374 J/cm

@Temperature 23.0 °C
0.400 - 0.700 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C