Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 87.2 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
Unannealed; ASTM D648
LyondellBasell Pro-faxâ„¢ SD183 Polypropylene Copolymer
Description: Pro-faxâ„¢ SD183 medium impact polypropylene copolymer resin is extremely resistant to aging at elevated temperatures in both wet and dry environments. It has an excellent balance of..
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
Unannealed; ISO 75B-1, -2
LyondellBasell Hostacomâ„¢ CB189FC/1 Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB189FC/1 medium melt flow, 1,300 MPa flexural modulus, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact, stiffne..
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
Unannealed; ASTM D648
Techmer ES HiFill® HIPS 484 GY
Availability: North AmericaForms: PelletsAppearance: GreyInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
Westlake Plastics HIPS High Impact Polystyrene, Compression Molded
Compression molded HIPS is a low cost plastic material that is easily machined and fabricated. It is frequently used for preproduction prototyping. HIPS is a FDA compliant use in food processing a..
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
Westlake Plastics HIPS High Impact Polystyrene
HIPS is a low cost plastic material that is easy to machine and fabricate. It is often specified for low strength structural applications when impact resistance, machinability, and low cost are req..
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
ExxonMobil HDPE HD 6909.19 High Density Polyethylene Copolymer Resin
Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ..
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
ExxonMobil HDPE HD 6909.65 High Density Polyethylene Copolymer Resin
Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ..
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ISO 75-2/B
ExxonMobil PP1063L1 Polypropylene Homopolymer
Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other ..
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
ExxonMobil PP8244E1 Polypropylene Homopolymer
Product Description: A high crystallinity, high impact copolymer resin designed for injection molded applications requiring excellent processing attributes.Availability: North America Features:Bala..
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
Unannealed; ASTM D648
Dow H349-02 Polypropylene Homopolymer Resin
H349-02 Polypropylene Resin intended for use in biaxial oriented (BOPP) film processes. This product can also be used in extrusion and thermoforming applications where improved melt strength is des..
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
Aclo Accucomp ABS ABS802L High Impact Grade
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
Aclo Accucomp ABS ABS812L High Impact Grade
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
Aclo Accucomp ABS ABS881L Clear Grade
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
Aclo Accucomp ABS ABS810L Medium Impact Grade
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
Aclo Accutech Polypropylene Copolymer CP0437M10CL Mica Reinforced Coupled
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
Americas Styrenics MC3650 High Heat Crystal Polystyrene
Product CharacteristicsImproved cycle times in hard to fill partsExcellent clarity with slight blue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsHousewaresConsumer..
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
Americas Styrenics STYRON® 693 High Heat Crystal Polystyrene
Product CharacteristicsHigh heat resistanceHigh tensile strengthHigh stiffnessFood Contact CompliantUL Classification 94 HBTypical ApplicationsPackaging/Foam disposablesConsumer electronicsInformati..
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C
189 °F
ASTM D648
Ineos H03G-01 Polypropylene Homopolymer
This is a homopolymer designed for tenter frame BOPP processing and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsFood packagingOverwrap..
Copyright © lookpolymers.com All Rights Reserved