Michelman® DigiPrime® 5100 Primer

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name DigiPrime®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® DigiPrime® 5100 Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Primer for digital printingUsage: DigiPrime® 5100 is a print primer which provides excellent adhesion of HP Indigo electro inks to treated films and paper. It adheres well to many synthetics, including soft vinyl. This product is designed for screen printing, but may also be applied via flexo and other methods.Application data: DigiPrime® 5100 has been developed specifically for screen printing. It may also be applied via flexo, gravure, rod or roll coating systems. For screen printing, the following is recommended: 1. Mesh size: 180 lines per cm/460 lines per inch. 2. Thread diameter nominal: 27 micron 3. Squeegee: 80 Durometer A 4. Tension: 20-30NInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.02 g/cc
1.00 - 1.02 g/cc
Volatiles 74.5 - 76.4 %
74.5 - 76.4 %
pH 8.0 - 9.0
8.0 - 9.0
Brookfield Viscosity 150 - 300 cP
150 - 300 cP
Spindle # 2, rpm 60
Descriptive Properties Value Comments
Appearance White to light yellow, opaque liquid