Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.012 - 0.025 cm/cm | 0.012 - 0.025 in/in | |
SABIC PP 578P Polypropylene Homopolymer for Injection Molding Product Description: PP 578P is a controlled rheology PP grade of medium molecular weight distribution suitable for injection molding applications. It gives consistent processability, good flow pr.. |
|||
Linear Mold Shrinkage | 0.020 - 0.025 cm/cm | 0.020 - 0.025 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® 12-000 PRE-ELEC 12-000 is a conductive thermoplastic compound based on a polyacetal copolymer. Conductivity is achieved by using special carbon black. In addition to a low resistivity PRE-ELEC 12-000 has a.. |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 4.00 mm |
0.015 - 0.025 in/in @Thickness 0.157 in |
10.0 mm wide molded rod; ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 3.17 mm |
0.015 - 0.025 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 4000 ET-1001 L Polyphthalamide (PPA), Impact Modified - Lubricated |
|||
Linear Mold Shrinkage | 0.020 - 0.025 cm/cm @Thickness 3.17 mm |
0.020 - 0.025 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 732 High Density Polyethylene (HDPE), Talc 30% |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 M2 Nylon 6 for injection molding, 2% molybdenum disulphide lubricated Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.020 - 0.025 cm/cm | 0.020 - 0.025 in/in | ASTM D955 |
PolyOne Lubri-Tech™ ATH-5KV/000 Acetal-Homopolymer, Aramid Fiber
(discontinued **) Description/Features:Aramid Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
Ineos H03G-03 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: ExtrusionFeatures: Ease of processingTypical applications: Oriented filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Amoco® 7942 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Excellent mold release, AntistaticTypical applications: Closures, Thin-walled rigid packagingComplies with FDA specification, Title 21, CFR .. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
Ineos H38G-01 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fadeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520.Typical pr.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Acctuf® 3950 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Low gloss, High melt flow, Low temp impact, NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below fro.. |
|||
Linear Mold Shrinkage | 0.018 - 0.025 cm/cm | 0.018 - 0.025 in/in | |
Lehmann & Voss LUVOCOM® 80-8268 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Linear Mold Shrinkage | 0.018 - 0.025 cm/cm | 0.018 - 0.025 in/in | |
Lehmann & Voss LUVOCOM® 80-8470 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, .. |
|||
Linear Mold Shrinkage | 0.018 - 0.025 cm/cm @Thickness 3.17 mm |
0.018 - 0.025 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company ESD A 700 A Low Density Polyethylene (LDPE), ESD Protection - Static Dissipative |
|||
Linear Mold Shrinkage | 0.018 - 0.025 cm/cm @Thickness 3.20 mm |
0.018 - 0.025 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 200 D UV Nylon 6/12 (PA); UV Stabilized |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 3.17 mm |
0.015 - 0.025 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 200 H SI 2 Impact-Modified Nylon 6/6 (PA), Silicone Lubricated - Impact Modified |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 3.20 mm |
0.015 - 0.025 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 200 TFE 10 HS Nylon 6/6 (PA) PTFE Lubricated - Heat Stabilized |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 3.17 mm |
0.015 - 0.025 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 200 H MS Impact-Modified Nylon 6/6 (PA), Impact Modified - Molybdenum Disulfide |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 3.20 mm |
0.015 - 0.025 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 200 TFE 10 Nylon 6/6 (PA), PTFE Lubricated |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 3.17 mm |
0.015 - 0.025 in/in @Thickness 0.125 in |
ASTM D 955 |
RTP Company RTP 2299 X 80218 Polyetheretherketone (PEEK), PTFE Lubricated |
|||
Linear Mold Shrinkage | 0.020 - 0.025 cm/cm @Thickness 3.20 mm |
0.020 - 0.025 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 2740 S-30A Saturated Styrenic Block Copolymer, General Purpose |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 3.20 mm |
0.015 - 0.025 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 2740 S-50A Saturated Styrenic Block Copolymer, General Purpose |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 2870 Thermoplastic Elastomer Elastocon® 2870 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2870 is FDA compliant and well suited for cons.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
Ineos H03G-01 Polypropylene Homopolymer This is a homopolymer designed for tenter frame BOPP processing and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsFood packagingOverwrap.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
Ineos H08U-00 Polypropylene Homopolymer, Fiber Grade Suggested fabrication methods: Fiber spinningFeatures: UV stable, High tenacityTypical applications: Geotextiles, Continuous filamentComplies with FDA specification, Title 21, CFR 177.1520.Typical p.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Accpro® 9346 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Long-term heat aging, High stiffness, Nucleated, UL RecognizedComplies with FDA specification, Title 21, CFR 177.1520.Typical applications: .. |
|||
Linear Mold Shrinkage | 0.018 - 0.025 cm/cm @Thickness 3.20 mm |
0.018 - 0.025 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 800 SI 2 DEL Acetal (POM); Silicone Lubricated |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Accpro® 9117 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Sheet; ExtrusionFeatures: Improved MVTR, Stain resistanceTypical applications: Film, Rigid packagingComplies with FDA specification, Title 21, CFR 177.1520.Typical pro.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
Ineos H13Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical prope.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Amoco® 6361 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; Blow moldingFeatures: Ease of processingTypical applications: Oriented film, Sheet, Fiber, Profile, Consumer productsComplies with FDA specification, Title .. |