Polymer Property : Izod Impact, Notched = 0.214 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.214 J/cm

@Temperature 23.0 °C
0.400 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide
Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.214 J/cm

@Temperature 23.0 °C
0.401 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Ovation Polymers Nemcon™ H ABS DP116P ABS
ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Network Polymers NPP 30-1800
Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
0.125 inch bar; ASTM D256
Network Polymers SAN 278 Medium Blue Tint
Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc.
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet)
Izod Impact, Notched 0.214 J/cm

@Thickness 3.17 mm
0.400 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 2100 HF  Polyetherimide (PEI) High Flow  (discontinued **)
High FlowComments:High FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this pro..
Izod Impact, Notched 0.214 - 1.28 J/cm
0.400 - 2.40 ft-lb/in
Average value: 0.364 J/cm Grade Count:16
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu..
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
I. Stern N2380 High Heat Crystal Polystyrene
Features:High Molecular WeightExcellent Optical PropertiesApplicationsOPSFoamed TraysThick Walled Injection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. St..
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
I. Stern WC-102 General Purpose Crystal Polystyrene
Features:Good Processing CharacteristicsUL Classification 94 HBExcellent Water ClarityComplies with FDA Title 21 CFR 177.1640ApplicationsExtrusion FoamDisplaysInformation provided by I. Stern & Co. ..
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D 638
Styrolution PS 1621 GPPS
Easy flow material with excellent moldabilityExcellent clarity and set-up timeInformation provided by Styrolution
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D 638
Styrolution PS 3600/3601 GPPS
Exceptional flow characteristicsGood for thin wall and complex partsUSP Class VI certifiedInformation provided by Styrolution
Izod Impact, Notched 0.214 J/cm
0.401 ft-lb/in
ASTM D256
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade
Durez 29502 B brown phenolic is a two stage, glass and mineral filled, special purpose molding material with improved mechanical and heat resistant properties. It is formulated for close tolerance ..
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar..
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene
DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman.
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar..
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene
DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman.
Izod Impact, Notched 0.214 J/cm

@Thickness 3.17 mm
0.400 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 199 X 85860 B Polypropylene (PP), High Gravity Compound
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene
DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman.
Izod Impact, Notched 0.214 J/cm
0.401 ft-lb/in
ASTM D256A
Total PPH 3825 Polypropylene, Injection Molding Grade
Easy flow injection molding homopolymerEasy Flow - FINA 3825 exhibits exceptionally easy flow characteristics.FDA - FINA 3825 complies with all applicable FDA regulations for food contact applicatio..
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene
DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman.
Izod Impact, Notched 0.214 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.401 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Diamond Polymers SAN 263 Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Asahi Kasei Thermofil P-40TC-1156 40% Talc Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Americas Styrenics MC3700 High Heat Crystal Polystyrene
Product CharacteristicsEasy filling of thin-walled partsExceptional mold releaseImproved cycle times in hard to fill partsFood Contact CompliantUL Classification 94HBUSP Class VITypical Applications..
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Americas Styrenics STYRON® 649D High Heat Crystal Polystyrene
Product CharacteristicsExcellent moldabilityExcellent gloss in coextrusionExcellent clarityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk ..
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Amco Amalloy® B1025 Polymer Alloy
Amco Amalloy B1025 is a clear performance copolymer with exceptional clarity and toughness.Clear, medium melt-flow.Information provided by Amco Plastic Materials.
Izod Impact, Notched 0.214 - 2.14 J/cm
0.400 - 4.00 ft-lb/in
Average value: 0.673 J/cm Grade Count:190
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Izod Impact, Notched 0.214 J/cm

@Thickness 3.17 mm
0.400 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 399 X 91042 Polycarbonate (PC), Thermally Conductive - Electrically Insulative
Izod Impact, Notched 0.214 J/cm

@Temperature 23.0 °C
0.400 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Formosa Plastics Formolene® 4111T Homopolymer Polypropylene
Homopolymer for Non-Wovens and Extrusion Coating Formolene® 4111T is a low viscosity, polypropylene homopolymer designed for extrusion coating, and Nonwoven applications. Its unique combination of ..