Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics CHO-SEAL® 6435 Conductive Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-SEAL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SEAL® 6435 Conductive Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Material of choice for high shielding effectiveness where NBC fluid resistance is needed; good performance in corrosive environments.Molded onlyRoHS CompliantInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 3.45 - 3.95 g/cc
3.45 - 3.95 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 73 - 87
73 - 87
ASTM D2240
Tensile Strength >= 1.38 MPa
>= 200 psi
ASTM D412
Elongation at Break <= 200 %
<= 200 %
ASTM D412
Tear Strength <= 13.1 kN/m
<= 75.0 pli
ASTM D624
Compression Set <= 40 %

@Temperature 100 °C,
Time 252000 sec
<= 40 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395, Method B
Thermal Properties Metric English Comments
Thermal Conductivity 1.80 W/m-K

@Pressure 2.07 MPa
12.5 BTU-in/hr-ft²-°F

@Pressure 300 psi
ASTM D5470
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flex TR10
Electrical Properties Metric English Comments
Volume Resistivity <= 0.0060 ohm-cm
<= 0.0060 ohm-cm
without pressure-sensitive adhesive; CEPS-0002
Shielding Effectiveness >= 85 dB

@Frequency 2.00e+9 Hz
>= 85 dB

@Frequency 2.00e+9 Hz
Plane Wave; Method 2, MIL-DTL-83528 Para. 4.6.12
>= 85 dB

@Frequency 1.00e+10 Hz
>= 85 dB

@Frequency 1.00e+10 Hz
Plane Wave; Method 2, MIL-DTL-83528 Para. 4.6.12
>= 100 dB

@Frequency 5.00e+8 Hz
>= 100 dB

@Frequency 5.00e+8 Hz
E-Field; Method 2, MIL-DTL-83528 Para. 4.6.12
>= 105 dB

@Frequency 1.00e+8 Hz
>= 105 dB

@Frequency 1.00e+8 Hz
E-Field; Method 2, MIL-DTL-83528 Para. 4.6.12
Descriptive Properties Value Comments
Binder EPDM
Filler Ag/Ni
Heat Aging <0.0125 ohm-cm
100°C for 48hrs; CEPS-0002
Users viewing this material also viewed the following: