Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYabs SS0 ABS, High Flow Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYelast TPE R44 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 484C High Impact Polystyrene
(discontinued **) STYRON® 484C high impact polystyrene resin, is typically used in refrigeration applications, appliances, containers, lids, furniture and profiles. It offers excellent low temperature toughness, exc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C @Thickness 3.20 mm |
189 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY CR7520 ASA General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | |
Ineos ABS Lustran® LGA-SF
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquir.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
Flint Hills AP6112-HS Impact Copolymer Polypropylene High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: appliance components, automotive interior trim, and consumer durables.Former Huntsma.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C @Thickness 6.40 mm |
189 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa FRABS-518 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmLow temperature impact resistanceApplications:Injection moldingPower tools accessoriesInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
LG Chemical LUPOL TE-5006K Thermoplastic Elastomer Alloy, Weather Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
LyondellBasell Astryn NXO-21001 Polypropylene Copolymer Key Features: high melt flow, medium modulus polypropylene copolymer, high flow, excellent processability, excellent colorabilityApplications: wire harnesses, housings, thin walled partsDescription:.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | Unannealed; ISO 75B-1, -2 |
LyondellBasell Hostacomâ„¢ CB189FC/1 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CB189FC/1 medium melt flow, 1,300 MPa flexural modulus, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact, stiffne.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C @Thickness 6.40 mm |
189 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® QP-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C @Thickness 6.40 mm |
189 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® SF-0505HWR MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ISO 75-2 |
Borealis Daplen™ EE115AE TPO Compound Daplen EE115AE is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | 0.125 inch; ASTM D648 |
PlastxWorld CEVIAN®-V 500 ABS Medium Impact ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
A. Schulman PP 3479-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Westlake Plastics HIPS High Impact Polystyrene, Compression Molded Compression molded HIPS is a low cost plastic material that is easily machined and fabricated. It is frequently used for preproduction prototyping. HIPS is a FDA compliant use in food processing a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
A. Schulman PP 3479-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ISO 75-2/B |
ExxonMobil PP1063L1 Polypropylene Homopolymer Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | Unannealed; ASTM Data |
Dow C702-20 Polypropylene Impact Copolymer Dow Polypropylene Impact Copolymer Resins are semi-crystalline thermoplastic materials that can provide a combination of desirable properties and affordability: low density; excellent chemical resis.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® 6646 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 66 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Aclo Accucomp ABS ABS812L High Impact Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Aclo Accucomp ABS ABS881L Clear Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
Americas Styrenics STYRON® 693 High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthHigh stiffnessFood Contact CompliantUL Classification 94 HBTypical ApplicationsPackaging/Foam disposablesConsumer electronicsInformati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | |
BASF Polystyrol® 2710 Impact Grade Polystyrene (Europe) Special high-impact grade for refrigerators and the packaging sector. Particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
A. Schulman PP 3479-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ISO 75-2 |
Borealis Daplen™ ED135AI TPO Compound Daplen ED135AI is a 10% mineral filled grade intended for injection molding. ED135AI offers very good balance in stiffness/impact strengthDaplen ED135AI has been developed especially for the car in.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
Samyang Triel® 5500 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5500 is an extrusion grade.Information provided by Samyang. |