Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.214 J/cm @Thickness 6.35 mm |
0.400 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CP - 51 KC General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 6.35 mm |
0.400 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CP - 51 KC General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.214 J/cm @Temperature 23.0 °C |
0.400 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | 0.125 inch bar; ASTM D256 |
Network Polymers SAN 278 Medium Blue Tint Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.214 - 0.694 J/cm | 0.400 - 1.30 ft-lb/in | Average value: 0.409 J/cm Grade Count:59 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
I. Stern N1841 General Purpose Crystal Polystyrene Features:Excellent Process PropertiesEasy FlowApplicationsDisplaysToys, CosmeticsAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. Stern & Co. Inc. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
I. Stern N2380 High Heat Crystal Polystyrene Features:High Molecular WeightExcellent Optical PropertiesApplicationsOPSFoamed TraysThick Walled Injection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. St.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Ineos H44N-00 Polypropylene Homopolymer H44N-00 is a high flow rate, nucleated polypropylene homopolymer designed for compounding and injection molding applications. The grade benefits from a high stiffness and isotropic shrinkage to help.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
M. Holland Company SA400 Styrene Acrylonitrile High clarityGood processabilityHigh stiffnessApplications: AppliancesCosmeticsHousehold goods |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D 638 |
Styrolution PS 3100/3101 GPPS Good balance of flow and set-up propertiesModerate heat resistanceUSP Class VI certifiedInformation provided by Styrolution |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D 638 |
Styrolution PS 3190/3191 GPPS Low residual styrene monomer contentGood balance of flow and set-up propertiesInformation provided by Styrolution |
|||
Izod Impact, Notched | 0.214 J/cm @Temperature -30.0 °C |
0.400 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Izod Impact, Notched | 0.214 J/cm @Temperature -30.0 °C |
0.400 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | |
Abatron AboWeld/AboCure 7812-2 Thixotropic Epoxy AboWeld/AboCure 7812-2 is an underwater and cold-weather structural and dielectric adhesive paste. It is a 2-component thixotropic epoxy compound for dry, wet, and cold applications. It has many spe.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256A |
Braskem CP360H Homopolymer Polypropylene Description: Narrow MWD, Low Smoke / CondensateApplications: Suggested Uses Include Fine Denier Spunbond Nonwovens, High-Speed Spinning - Continuous Filament YarnThis resin meets the requirements fo.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Americas Styrenics EA3130 High Heat Crystal Polystyrene Product CharacteristicsAdditive FreeFood Contact CompliantTypical ApplicationsMedical PartsColor Concentrate CarrierLow Profile AdditivesInformation provided by AmericasStyrenics LLC. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Americas Styrenics STYRON® 675 High Heat Crystal Polystyrene Product CharacteristicsHigh heatMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsThin-walled partsInformation provided by AmericasStyrenics LLC. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Americas Styrenics STYRON® 686E High Heat Crystal Polystyrene Product CharacteristicsExceptional balance between heat resistance, toughness and flowGood dimensional stability and excellent clarityFood Contact CompliantTypical ApplicationsFoamed PS sheets used .. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Americas Styrenics STYRON® 693 High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthHigh stiffnessFood Contact CompliantUL Classification 94 HBTypical ApplicationsPackaging/Foam disposablesConsumer electronicsInformati.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | 0.5 x 0.125 in.; ASTM D256 |
Americas Styrenics STYRON™ 668 General Purpose Polystyrene Resin STYRON™ 668 is a general purpose polystyrene with medium flow and a balance of heat resistance and stiffness characteristics that make it suitable for applications such as CD jewel boxes. STYRON™.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Asahi Kasei Thermofil P-20TC-1161 20% Talc Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Amco Amalloy® B1025 Polymer Alloy Amco Amalloy B1025 is a clear performance copolymer with exceptional clarity and toughness.Clear, medium melt-flow.Information provided by Amco Plastic Materials. |
|||
Izod Impact, Notched | 0.214 - 2.14 J/cm | 0.400 - 4.00 ft-lb/in | Average value: 0.673 J/cm Grade Count:190 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Notched | 0.214 J/cm @Temperature 23.0 °C |
0.400 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Formosa Plastics Formolene® 4111T Homopolymer Polypropylene Homopolymer for Non-Wovens and Extrusion Coating Formolene® 4111T is a low viscosity, polypropylene homopolymer designed for extrusion coating, and Nonwoven applications. Its unique combination of .. |
|||
Izod Impact, Notched | 0.214 - 1.49 J/cm | 0.400 - 2.80 ft-lb/in | Average value: 0.523 J/cm Grade Count:25 |
Overview of materials for Polypropylene with 30% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Izod Impact, Notched | 0.214 - 1.07 J/cm | 0.400 - 2.00 ft-lb/in | Average value: 0.442 J/cm Grade Count:24 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |