Material Notes:
50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM-D638
Tensile Modulus 2.00 GPa
290 ksi
ASTM-D638
Flexural Yield Strength 61.0 MPa
8850 psi
ASTM-D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM-D790
Izod Impact, Notched 0.910 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
1.70 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM-D256
1.60 J/cm

@Thickness 3.20 mm,
Temperature -18.0 °C
3.00 ft-lb/in

@Thickness 0.126 in,
Temperature -0.400 °F
ASTM-D256
2.99 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
5.60 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM-D256
Impact Test 18.0 J

@Temperature -40.0 °C
13.3 ft-lb

@Temperature -40.0 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763
19.0 J

@Temperature -40.0 °C
14.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Total Energy; ASTM-D3763
23.0 J

@Temperature -18.0 °C
17.0 ft-lb

@Temperature -0.400 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763
26.0 J

@Temperature -18.0 °C
19.2 ft-lb

@Temperature -0.400 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Total Energy; ASTM-D3763
31.0 J

@Temperature 23.0 °C
22.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763
43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Total Energy; ASTM-D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
Unannealed; ASTM-D648
Optical Properties Metric English Comments
Gloss 40 %
40 %
Formed, Angle 60°; ASTM-D523
85 %
85 %
Sheet, Angle 60°; ASTM-D523