Polymer Property : Impact Test = 31.7 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Total Energy; ASTM-D3763
Ineos ABS Lustran® 256/Lustran® 752 Blended ABS Resin
50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS
Impact Test 43.0 J

@Temperature -30.0 °C
31.7 ft-lb

@Temperature -22.0 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics Noryl GTX GTX904 PPE+PS+PA
Unreinforced; improved processing; excellent chemical resistance; 320F (160C) HDT.This data was supplied by SABIC-IP for the Americas region.
Impact Test 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
Diamond Polymers Centrex® 833 Sheet Extrusion Grade
Centrex 833 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it ..