Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.99 J/cm @Thickness 3.17 mm |
5.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trilac® ABS-HH2000 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.99 J/cm @Thickness 3.17 mm |
5.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trilac® ABS-HS5500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.99 J/cm @Thickness 3.17 mm |
5.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trilac® ABS-HF5500 High Flow ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.99 J/cm @Thickness 3.17 mm |
5.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Global ABS-HI-121 High Impact ABS Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 2.99 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
5.60 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM-D256 |
Ineos ABS Lustran® 256/Lustran® 752 Blended ABS Resin 50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS |
|||
Izod Impact, Notched | 2.99 J/cm @Temperature 4.00 °C |
5.60 ft-lb/in @Temperature 39.2 °F |
1/8'' notched bar, partial failure, (refrigerator temperature); ASTM D256 |
Ineos R01C-01 Polypropylene Random Copolymer This is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding. Applications that require good see-through clarity combined with good heat resistance .. |
|||
Izod Impact, Notched | 2.99 J/cm @Temperature -40.0 °C |
5.60 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 1101 PBT+PC (Asia Pacific) Unreinforced, opaque polycarbonate/polyester alloy. Excellent low temperature impact plus chemical resistance to automotive fluid.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 2.99 J/cm @Temperature -40.0 °C |
5.60 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 5220 PBT+PC (Asia Pacific) Unreinforced, polycarbonate-based polymer blend, excellent chemical resistance and impact.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 2.99 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.60 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS NAT Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.99 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.60 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 92RK Availability: North AmericaForms: PelletsFeatures: General PurposeProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.99 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.60 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS LE BK Availability: North AmericaForms: PelletsFeatures: Low ExtractablesAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.99 J/cm @Thickness 3.17 mm |
5.60 ft-lb/in @Thickness 0.125 in |
|
TPI Porene® ABS-GA800 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.99 J/cm @Thickness 3.17 mm |
5.60 ft-lb/in @Thickness 0.125 in |
|
TPI Porene® ABS-GA850 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.99 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.60 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8008 Availability: North AmericaForms: PelletsFeatures: General Purpose Appearance: Natural ColorInformation provided by TP Composites, Inc. |