Impact Test 23.0 J

@Temperature -18.0 °C
17.0 ft-lb

@Temperature -0.400 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763
Ineos ABS Lustran® 256/Lustran® 752 Blended ABS Resin
50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS