Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0148 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L7416 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion LR840 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
PolyOne Geon™ Vinyl Rigid Molding M5005 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding MR840 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 23.0 °C |
3.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® X17 ABS Automotive: Very high heat resistance with high strength and modulus. UL94 HB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | >= 1.60 J/cm @Temperature 23.0 °C |
>= 3.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 8300K (EPT30R) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature -40.0 °C |
3.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant Contains UV absorber.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 0.000 °C |
3.00 ft-lb/in @Temperature 32.0 °F |
injection molded specimen; ASTM D256 |
Phillips Sumika Marlex® AGM-110 Reactor Thermoplastic Polyolefins, Cold Temperature Impact Resistant
(discont Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. .. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM-D256 |
Ineos ABS Lustran® 256 Extrusion Blending Grade Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi.. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 23.0 °C |
3.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ineos L06Z-00 Polypropylene Impact Copolymer This is a medium MFR impact copolymer polypropylene made for injection molded caps and closures applications. It offers a good balance of stiffness to impact resistance as compared to other impact .. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF13 IM-1 HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF13 IM2 HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8004 FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp.. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature -30.0 °C |
3.00 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX904 PPE+PS+PA Unreinforced; improved processing; excellent chemical resistance; 320F (160C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Asia Pacific) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature -40.0 °C |
3.00 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PX1701 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 0.000 °C |
3.00 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Formosa Plastics Formolene® 6575N Impact Copolymer Polypropylene Impact Copolymer for High Speed injection Molded Applications Formolene® 6575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging,.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 0.000 °C |
3.00 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 0820 HT Acrylonitrile Butadiene Styrene ABS with high thermal resistanceGood impact resistance, stiffness, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers Centrex® 821 ASA Weatherable Polymers Injection Molding Grade Centrex 821 resin is a medium-gloss, high-heat, medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and pr.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D-256 |
Axiall Suprel® SVA 9412 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 inclu.. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 23.0 °C |
3.00 ft-lb/in @Temperature 73.4 °F |
50%RH; ASTM D256 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 23.0 °C |
3.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 23.0 °C |
3.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 0.000 °C |
3.00 ft-lb/in @Temperature 32.0 °F |
injection molded specimen; ASTM D256 |
Phillips Sumika Marlex® ABF-110 Reactor Thermoplastic Polyolefin, Cold Temperature Impact Resistant
(disconti Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. .. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN®-V T150 ABS Medium impact transparent ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |