Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87416 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0148 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L7416 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L7416 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5200 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5705 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 22.8 °C |
3.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ HTX M6215 Polyvinyl Chloride Alloy (PVC Alloy) It is recommended that the compound pellets be dried for 3 to 4 hours at 150 deg. F.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 0.000 °C |
3.00 ft-lb/in @Temperature 32.0 °F |
injection molded specimen; ASTM D256 |
Phillips Sumika Marlex® AGM-110 Reactor Thermoplastic Polyolefins, Cold Temperature Impact Resistant
(discont Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. .. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.20 mm, Temperature -18.0 °C |
3.00 ft-lb/in @Thickness 0.126 in, Temperature -0.400 °F |
ASTM-D256 |
Ineos ABS Lustran® 256/Lustran® 752 Blended ABS Resin 50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 23.0 °C |
3.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ineos L06Z-00 Polypropylene Impact Copolymer This is a medium MFR impact copolymer polypropylene made for injection molded caps and closures applications. It offers a good balance of stiffness to impact resistance as compared to other impact .. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF13 IM2 HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF14 IM HS L BK 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8004 FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp.. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature -30.0 °C |
3.00 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX904 PPE+PS+PA Unreinforced; improved processing; excellent chemical resistance; 320F (160C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Asia Pacific) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature -18.0 °C |
3.00 ft-lb/in @Temperature -0.400 °F |
ASTM D256 |
Formosa Plastics Formolene® 2706N Impact Copolymer Polypropylene Copolymer for Heavy Duty Injection Molded Applications Formolene® 2706N is a copolymer of polypropylene designed and formulated for injection molding applications. It contains a unique combination .. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 0.000 °C |
3.00 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Formosa Plastics Formolene® 6575N Impact Copolymer Polypropylene Impact Copolymer for High Speed injection Molded Applications Formolene® 6575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging,.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 0.000 °C |
3.00 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 0820 HT Acrylonitrile Butadiene Styrene ABS with high thermal resistanceGood impact resistance, stiffness, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 0.000 °C |
3.00 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 2020 MT Acrylonitrile Butadiene Styrene ABSMedium heat resistance, good impact resistance, good melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac ABS Acrylonitrile Butadiene Styrene |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 23.0 °C |
3.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem CP 195 Injection Molding Polypropylene Description: CP 195 is a very high melt flow rate heterophasic copolymer developed for high speed injection moulding machines and high productivity thin-walled injection moulded parts. The product f.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 6.35 mm |
3.00 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 9153 Rigid PVC, Molding Georgia Gulf 9153 is an excellent combination of chemical resistance, impact and processing for chemically active products, such as pine oil cleaners.Information provided by Georgia GulfGeorgia Gulf.. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 23.0 °C |
3.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 0.000 °C |
3.00 ft-lb/in @Temperature 32.0 °F |
injection molded specimen; ASTM D256 |
Phillips Sumika Marlex® ABF-110 Reactor Thermoplastic Polyolefin, Cold Temperature Impact Resistant
(disconti Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. .. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 2512 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |