Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.910 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.70 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87549 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.910 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
1.70 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5705 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastalloy DA510 Polymer
(discontinued **) Eastalloy Polymer DA510 is a clear copolyester/polycarbonate alloy. This product has good physical properties. These include good impact strength, chemical resistance, heat resistance, dimensional s.. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastalloy MA510 Polymer
(discontinued **) Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhan.. |
|||
Izod Impact, Notched | 0.910 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.70 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM-D256 |
Ineos ABS Lustran® 256/Lustran® 752 Blended ABS Resin 50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS |
|||
Izod Impact, Notched | 0.910 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.70 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM-D256 |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -20.0 °C |
1.70 ft-lb/in @Temperature -4.00 °F |
ASTM D 256 |
MRC Polymers SATRANâ„¢ 805 ABS Terpolymer, Impact Modified Information provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c.. |
|||
Izod Impact, Notched | 0.910 J/cm @Temperature -40.0 °C |
1.70 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |