Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 19.0 J @Temperature 23.0 °C |
14.0 ft-lb @Temperature 73.4 °F |
multiaxial, at 2.2 m/sec, 100% ductile; ASTM 3763 |
S&E Specialty Polymers TufFill™ 5008 Polyolefin Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p.. |
|||
Impact Test | 19.0 J @Temperature 23.0 °C |
14.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 725.21 Molding, extrusion, compounding and adhesive resin
(discontinued **) Escorene Ultra LD 722.21 is 18 wt% vinyl acetate copolymer suitable for molding, extrusion, compounding and hot melt adhesive applications.Information provided by ExxonMobil Chemical |
|||
Impact Test | 19.0 J @Temperature -40.0 °C |
14.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Total Energy; ASTM-D3763 |
Ineos ABS Lustran® 256/Lustran® 752 Blended ABS Resin 50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS |
|||
Impact Test | 19.0 J @Temperature -18.0 °C |
14.0 ft-lb @Temperature -0.400 °F |
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763 |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Impact Test | 19.0 J @Temperature 23.0 °C |
14.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 705.MJ Molding, extrusion and compounding resin Escorene Ultra LD 705.MJ is a fraction melt index, 13.3 wt% vinyl acetate copolymer suitable for use in making blow molded articles, extruded profiles and compounds.Information provided by ExxonMobi.. |
|||
Impact Test | 19.0 J @Temperature 23.0 °C |
14.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 761.36 Molding, extrusion and compounding resin Escorene Ultra LD 761.36 is a 26.7% vinyl acetate copolymer excellent flexibility and low temperature toughness. LD 761.36 has high filler acceptance.Availability: Latin America, North America and S.. |