Ovation Polymers Nemcon™ E PET 30131 PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Ovation Polymers
Trade Name Nemcon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Nemcon™ E PET 30131 PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PET-Fiber Grade with ESD Range Conductivity with improved processability. Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 52.0 MPa
7540 psi
50 mm/min; ASTM D638
Elongation at Break 2.6 %
2.6 %
50 mm/min; ASTM D638
Tensile Modulus 2.55 GPa
370 ksi
50 mm/min; ASTM D638
Flexural Strength 90.0 MPa
13100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.09 GPa
448 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.200 J/cm

@Temperature 23.0 °C
0.375 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Electrical Properties Metric English Comments
Surface Resistivity per Square 31000 ohm
31000 ohm
ASTM D257