Material Notes:
Modified BMI film adhesive, superior strength to 550°F / 288°C. Moisture resistant, processes like conventional high temperature epoxies. Minimum order required. Data from 0.10 psf, 500 g / m2.Applications: Composite Bonding Metal and Honeycomb Bonding
Physical Properties Metric English Comments
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Tensile Strength 4.10 MPa
595 psi
Flatwise
Adhesive Bond Strength 13.8 MPa

@Temperature -55.0 °C
2000 psi

@Temperature -67.0 °F
Lap Shear
13.8 MPa

@Temperature 25.0 °C
2000 psi

@Temperature 77.0 °F
Lap Shear
15.2 MPa

@Temperature 260 °C
2200 psi

@Temperature 500 °F
Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 288 °C
550 °F
Glass Transition Temp, Tg 210 °C
410 °F
wet
298 °C
568 °F
dry
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 177 °C
1.00 hour

@Temperature 351 °F
Descriptive Properties Value Comments
Honeycomb Climbing Drum Peel, mN/m 15
at 25°C
Out-Time (days) 30
at 25°C