Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Anderman Ceramics EZC96P Zirconia, 96%, Calcia-Stabilized

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer Anderman Ceramics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Anderman Ceramics EZC96P Zirconia, 96%, Calcia-Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in impervious or porous grades in a range of shapes and sizes.Information provided by Anderman Ceramics.
Physical Properties Metric English Comments
Density 4.30 g/cc
0.155 lb/in³
Open Porosity 25 %
25 %
Thermal Properties Metric English Comments
CTE, linear 9.60 µm/m-°C
5.33 µin/in-°F
Thermal Conductivity 2.00 W/m-K

@Temperature 20.0 - 100 °C
13.9 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Maximum Service Temperature, Air 2400 °C
4350 °F
Component Elements Properties Metric English Comments
CaO 4.0 %
4.0 %
ZrO2 96 %
96 %
Descriptive Properties Value Comments
Thermal Shock Resistance Good
Copyright © lookpolymers.com All Rights Reserved