Material Notes:
Homopolymer, UL certified, and FDA compliant.Features: Nucleated, antistat, and clarified.Applications: Injection molding: high clarity, housewares, and syringes, for EO sterilization.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength, Yield 39.0 MPa
5660 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.62 GPa
235 ksi
1% Secant; ASTM D790
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
23° C; ASTM D256
Gardner Impact 1.00 J
0.738 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648