Material Notes:
86155 is a flexible (90A durometer) vinyl compound formulated from FDA-santioned raw materials. This compound has received NSF Standard 61 only for sheets applications.NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high water content only. This material is also listed under NSF Std. 61. This listing covers many uses and restrictions may apply depending on the application. It is the customer's responsibility to ensure that the compound is suitable for its intended application. Please contact us to review the suitability of specific products in specific applications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
15 sec; ASTM D2240
90
90
ASTM D2240
Tensile Strength at Break 18.3 MPa
2650 psi
Type IV, 510 mm/min; ASTM D638
Tensile Strength 10.7 MPa

@Strain 100 %
1550 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 400 %
400 %
Type IV, 510 mm/min; ASTM D638
Tear Strength 76.2 kN/m
435 pli
Die C, 510 mm/min; ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -27.0 °C
-16.6 °F
ASTM D746
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
NSF 61
Features Food Contact Acceptable
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved