Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 15.2 MPa @Temperature 260 °C |
2200 psi @Temperature 500 °F |
Lap Shear |
Henkel Hysol EA 9673 (BMI) Film Adhesive Modified BMI film adhesive, superior strength to 550°F / 288°C. Moisture resistant, processes like conventional high temperature epoxies. Minimum order required. Data from 0.10 psf, 500 g / m2.. |
|||
Adhesive Bond Strength | 15.2 MPa @Temperature -55.0 °C |
2200 psi @Temperature -67.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9390 Paste Adhesive System Low viscosity system for high temperature wet lay-up composite repair. Qualified to BMS 8-301.Applications: Structural Bonding Low Viscosity Wet Lay-Up Composite Bonding |
|||
Adhesive Bond Strength | 15.2 MPa @Temperature 25.0 °C |
2200 psi @Temperature 77.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 960F Paste Adhesive System Fast-set fairing and smoothing compound for exterior aircraft surfaces.Sandable after 6 hours |