Mechanical Properties Metric English Comments
Adhesive Bond Strength 13.8 MPa

@Temperature -55.0 °C
2000 psi

@Temperature -67.0 °F
Lap Shear
Henkel Hysol EA 9673 (BMI) Film Adhesive
Modified BMI film adhesive, superior strength to 550°F / 288°C. Moisture resistant, processes like conventional high temperature epoxies. Minimum order required. Data from 0.10 psf, 500 g / m2..
Adhesive Bond Strength 13.8 MPa

@Temperature 25.0 °C
2000 psi

@Temperature 77.0 °F
Lap Shear
Henkel Hysol EA 9673 (BMI) Film Adhesive
Modified BMI film adhesive, superior strength to 550°F / 288°C. Moisture resistant, processes like conventional high temperature epoxies. Minimum order required. Data from 0.10 psf, 500 g / m2..
Adhesive Bond Strength 13.8 MPa

@Temperature 121 °C
2000 psi

@Temperature 250 °F
Lap Shear
Henkel Hysol EA 9696 Film Adhesive
Second generation, moisture-resistant, toughened 250°F / 121°C service, modified epoxy film. Qualified to BMS 5-101 and BMS 5-129. Data from .060 psf, 300 g / m2.Applications: Composite Bondin..
Adhesive Bond Strength 13.8 MPa

@Temperature 93.0 °C
2000 psi

@Temperature 199 °F
Tensile Lap Shear
Henkel Hysol EA 934NA Paste Adhesive System
Two part adhesive system with superior strengthCures at room temperatureApplications: Potting Structural Repair Liquid Shim
Adhesive Bond Strength 13.8 MPa

@Temperature 93.0 °C
2000 psi

@Temperature 199 °F
Tensile Lap Shear
Henkel Hysol EA 9377 Paste Adhesive System
Moldable plastic shim, excellent microcracking resistance under thermal cycling. High compressive strength.Application: Liquid Shim
Adhesive Bond Strength 13.8 MPa

@Thickness 1.50 mm
2000 psi

@Thickness 0.0591 in
Lap Shear (CRS St 1203); EN 1465
Dow BETAMATE™ XW 1185 Epoxy
BETAMATE™ XW 1185 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel and aluminum, is resi..
Adhesive Bond Strength 13.8 MPa

@Temperature 23.9 °C
2000 psi

@Temperature 75.0 °F
on steel; ASTM D1002-64
3M Pronto™ CA-9 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A slower setting version of CA-..
Adhesive Bond Strength 13.8 MPa

@Temperature 23.9 °C
2000 psi

@Temperature 75.0 °F
on steel; ASTM D1002-64
3M Pronto™ CA-100 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Toughened material that provide..
Adhesive Bond Strength 13.8 MPa

@Temperature 23.9 °C
2000 psi

@Temperature 75.0 °F
on steel; ASTM D1002-64
3M Pronto™ CA-5 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A high viscosity, slower settin..
Adhesive Bond Strength 13.8 MPa

@Temperature 23.9 °C
2000 psi

@Temperature 75.0 °F
on steel; ASTM D1002-64
3M Pronto™ CA-50 Gel Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A high-viscosity gel consistenc..
Adhesive Bond Strength 13.8 MPa

@Temperature 23.9 °C
2000 psi

@Temperature 75.0 °F
on steel; ASTM D1002-64
3M Pronto™ CA-8 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Fast setting adhesive with exce..
Adhesive Bond Strength 13.8 MPa

@Temperature 100 °C
2000 psi

@Temperature 212 °F
Lap Shear Strength vs. Aluminum
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
Adhesive Bond Strength 13.8 MPa

@Temperature 177 °C
2000 psi

@Temperature 351 °F
Lap Shear
Henkel Hysol EA 9257 Primer
Waterborne, corrosion-inhibiting primer, maintains surface bondability after multiple prebonding cure cycles. Meets SCAQMD Rule 1124. Replacement for Hysol EA 9210B.Applications: Sprayable Low Visc..
Adhesive Bond Strength 13.8 MPa

@Temperature -55.0 °C
2000 psi

@Temperature -67.0 °F
Lap Shear
Henkel Hysol EA 9396.6MD Paste Adhesive System
Cure syntactic, with excellent high temperature properties. Applications: Potting Syntactic
Adhesive Bond Strength 13.8 MPa

@Temperature 121 °C
2000 psi

@Temperature 250 °F
Lap Shear
Henkel Hysol EA 9628 Film Adhesive
First generation, modified epoxy film, good stress, environmental resistance and structural propertiesApplications: Composite Bonding, Metal & Honeycomb BondingData from .060 psf, 300 g/m2
Adhesive Bond Strength 13.8 MPa

@Temperature 93.0 °C
2000 psi

@Temperature 199 °F
Tensile Lap Shear
Henkel Hysol EA 9396/C-2 Paste Adhesive System
Two-part, elevated cure, unfilled, low viscosity adhesive with structural properties to 400°F / 204°C.Applications: Structural Repair Low Viscosity Wet Lay-Up Composite Bonding
Adhesive Bond Strength 13.8 MPa

@Temperature -55.0 °C
2000 psi

@Temperature -67.0 °F
Tensile Lap Shear
Henkel Hysol EA 960F Paste Adhesive System
Fast-set fairing and smoothing compound for exterior aircraft surfaces.Sandable after 6 hours