Material Notes:
Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according to the required surface properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1750 ppmSlip: NoThermal Stabilizer: YesInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ExxonMobil method
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 1750 ppm
1750 ppm
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 200 %
200 %
ASTM D882
Film Elongation at Break, TD 510 %
510 %
ASTM D882
Elmendorf Tear Strength MD 180 g
180 g
ASTM D1922
Elmendorf Tear Strength TD 150 g
150 g
ASTM D1922
Dart Drop Test 230 g
0.507 lb
ASTM D1709A
Film Tensile Strength at Break, MD 22.1 MPa
3200 psi
ASTM D882
Film Tensile Strength at Break, TD 19.3 MPa
2800 psi
ASTM D882
1% Secant Modulus, MD 159 MPa
23000 psi
ASTM D882
1% Secant Modulus, TD 179 MPa
26000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 223 °C
<= 433 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 70 %
70 %
45°; ASTM D2457