Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, MD = 3200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 22.1 MPa
3200 psi
ASTM D882
LyondellBasell Petrothene® NA952000 Low Density Polyethylene
ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process..
Film Tensile Strength at Break, MD 22.1 MPa
3200 psi
ASTM D882
LyondellBasell Petrothene® NA952094 Low Density Polyethylene
ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process..
Film Tensile Strength at Break, MD 22.1 MPa
3200 psi
ASTM D882
LyondellBasell Petrothene® NA480145 Low Density Polyethylene
ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low..
Film Tensile Strength at Break, MD 22.1 MPa
3200 psi
ASTM D882
LyondellBasell Petrothene® NA480177 Low Density Polyethylene
ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low..
Film Tensile Strength at Break, MD 22.1 MPa
3200 psi
ASTM D882
LyondellBasell Petrothene® NA480178 Low Density Polyethylene
ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low..
Film Tensile Strength at Break, MD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LD 141.87 Shrink Film Resin
LD 141.87 is a vinyl acetate copolymer film resin with very good toughness and shrink properties. Applications include Medium duty shrink wrap and Heavy duty bags.Information provided by ExxonMobil..
Film Tensile Strength at Break, MD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin
Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi..
Film Tensile Strength at Break, MD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 313.NF Low Density Polyethylene Resin
Product Description: LD 313.NF is a 3 % vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopoly..
Film Tensile Strength at Break, MD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 368HD Low Density Polyethylene Resin
Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according..
Film Tensile Strength at Break, MD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 368ON Low Density Polyethylene Resin
Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according..
Film Tensile Strength at Break, MD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate
Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It produces a so..