Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 2018CA Blown Film Resin
(discontinued **) Exceed 2018CA resin is an ethylene based polymer produced with metallocene single site catalysts using ExxonMobil Chemicals EXXPOL® Technology. The higher melt index makes this polymer ideally sui.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018 DA Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018 FA Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
Westlake EF444 4.7% Ethylene Vinyl Acetate Copolymer
(discontinued **) Excellent haze and gloss, excellent impact strength and very good sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, section 177.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
Westlake EF608 Low Density Polyethylene Westlake EF608 is a high melt index LDPE resin suggested for thin gauge garment films and other films requiring excellent drawdown. The high melt index makes this material a good choice in compound.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
Westlake Elevate™ EF439 4.0% Ethylene Vinyl Acetate Copolymer Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | Cast Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7114 Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for applications that require: Good stiffness at thin gaugesGood drawdownExcellent processabilityCan use straight or in blends with L.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 2018CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018CA is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films as well as skin layer in coex.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 2018HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018HA is a metallocene Catalyzed ethylene-hexene copolymer. Films made from Exceed 2018HA have outstanding tensile, impact strength, and puncture. These superior strengt.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 313.NF Low Density Polyethylene Resin Product Description: LD 313.NF is a 3 % vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopoly.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 361BW Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 361JD Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 362BR Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 362BW Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 362HE Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 362ON Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 363BW Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 368HD Low Density Polyethylene Resin Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil LDPE LD 368ON Low Density Polyethylene Resin Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according.. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018EB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018EB have outstanding tensile, impact, puncture resistance and low temperature properties. .. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018 EA Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018 EB Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
1% Secant Modulus, TD | 179 MPa | 26000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018 CA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018CA have outstanding tensile, puncture resistance and very good sealing properties. These.. |