Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Polymer Industries Densetec LDPE Sheet Polymer Industries Densetec LDPE is a material that`s soft, flexible, and tough, even at low temperatures. Because of the fact that Densetec LDPE has very good formability traits and is very pliable.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D4883 |
ExxonMobil Escorene® LL-6101 LLDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Medium Flow, High Gloss, Excellent ImpactUses: Large houseware containers, General purpose injection molding |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin; 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-1117 LLDPE Film/Sandwich Bag Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin. Films made from LL-1117 have very good tensile properties and toughness. This resin's good strength and drawability all.. |
|||
Density | 0.924 - 0.928 g/cc | 0.0334 - 0.0335 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) Arak 0410AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Chevron Phillips KN 226B LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Excellent Mold Release, Mode.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Chevron Phillips 5758 LDPE High Clarity, High Impact Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: High Clarity, Excellent Impact Strength, Medium Slip, Medium Antiblock, Moderately High Coefficient of Friction, Easy Openability of BagsApplications:Case Shr.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ExxonMobil Method |
ExxonMobil LD 071.MU Blown Film Resin
(discontinued **) LD 071 series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, toughness, burn-through re.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D1505 |
M. Holland Company LD700 LDPE
(discontinued **) Features: High Clarity, High Flow, Narrow Molecular Wt. Dist., Good Processability, Warp ResistantUses: Closure Caps, Drink LidsApprovals: FDA 21 CFR 177.1520(c) 2.2 and ASTM D 1248, I, Class A, Cat.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® LF-0225-B LDPE Clarity Film Resin
(discontinued **) Features: High optical clarityExcellent processability Applications: Produce and bakery filmLinersTextile packaging filmGeneral packaging requiring high clarity filmInformation provided by Nova Chem.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D792 |
DuPont Bynel® 3095 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Huntsman PE1407 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | |
LyondellBasell Lupolen® 2410 T LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (0.5 mil Film) ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die b.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) 2404TC47 Low Density Polyethylene LDPE 2404TC47 Light duty FilmIt is used for very thin films requiring good optical properties for general packaging applications e.g. covering film with very low blocking tendency.Information provi.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) 2501TN00 Low Density Polyethylene LDPE 2501TN00 Hygienic Film It is used in diaper film, lamination film and in applications where low blocking behavior without the help of additives is required.Information provided by Iran Petroch.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5069 400 Micron LLDPE Powder Description: ICOFLO 510-5069 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5071 800 Micron LLDPE Powder Description: ICOFLO 510-5071 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) LT0470/KJ Low Density Polyethylene LT0470/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. Application: stiffer thin films for textile p.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D792 - ISO 1183 |
DuPont Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3117 AC is intended for coextrusion and compounding. Due to its high melt flow rate, it is used also in extrusion coating. Elvaloy® 3117 AC is soft, flexible and has good adhesion to va.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil Method |
ExxonMobil LD 312.09 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 306.75 Low Density Polyethylene Resin Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.Availability: Latin A.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 312.82 Low Density Polyethylene Resin Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior.. |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 368ON Low Density Polyethylene Resin Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 1201KG Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1201 series are LLDPE grades, offering excellent combination of stiffness and optical properties (when blended with 10-20% LDPE) Availability: Africa & Middle East, Asia Paci.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2083G Linear Low Density Polyethylene Excellent tear strength, outstanding toughness Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D792 |
Aclo Accucomp Polyethylene LD0102L Low Density |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM-D792 |
Braskem LL6802N LLDPE Blown Film Extrusion Polyethylene Copolymer LL6802N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing aid .. |