Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Palm Labs Adhesives Turbo Fuse Series 440 (GEL) Rapid Bonding Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Palm Labs Adhesives
Trade Name TURBO FUSE SERIES
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Palm Labs Adhesives Turbo Fuse Series 440 (GEL) Rapid Bonding Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE 280 SERIES SEMI-GEL advanced thixotropic formula is designed to polymerize instantly by absorbing surface moisture. The product's performance has been tested with a variety of materials, and is recommended for a multitude of applications. The fast curing qualities make it especially desirable in high speed industrial production. TURBO FUSE SERIES 280 SEMI-GEL is ideal for use in applications that require a gel like adhesive that will flow out of a bottle. Because of the thick gel consistency, it works especially well in poor fitting applications such as rough metal or ceramic repair, unfinished metal to metal bonding, and metal to rubber. Because of the thick gel consistency, it works especially well in poor fitting applications such as rough metal or ceramic repair, unfinished metal to metal bonding, and metal to rubber.Part Numbers for this data: 07-280, 10-280, 15-280, 20-280, 30-280Soluble in Acetone, MEK, Amide, Methylene ChlorideInformation provided by Palm Laboratories Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Liquid State
Mechanical Properties Metric English Comments
Hardness, Barcol 65
65
Cured State
Shear Strength 17.2 MPa
2500 psi
Tensile, (Cured State)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.2 °C
180 °F
Cured State
Softening Point 149 °C
300 °F
Cured State
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Cured State
Flash Point 76.7 - 93.3 °C
170 - 200 °F
Liquid State (Tagliabue closed cup)
Electrical Properties Metric English Comments
Dielectric Constant 3.33

@Frequency 1.00e+6 Hz
3.33

@Frequency 1.00e+6 Hz
Cured State
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Liquid State
Descriptive Properties Value Comments
Appearance Clear white gel
Liquid State
Clear-Hard
Cured State
Base compound (Resin) Ethyl Cyanoacrylate
Liquid State
Gap Fill 0.010"
Cured State
Material Set Up Time <90 sec
Phenolic to Phenolic
10-25 sec
Rubber to Rubber
20-30 sec
Aluminum to Aluminum
50-100 sec
Steel to Steel
50-70 sec