Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 223 - 225 °C | 433 - 437 °F | |
Plastcom SLOVASTER® B/A GF 30 PBT, 30% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Melting Point | 223 °C | 433 °F | ISO 3146 |
PolyOne Bergamid™ B650 G/Mi20 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melting Point | 223 °C | 433 °F | ISO 3146 |
PolyOne Bergamid™ B70 red RAL3001 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melting Point | 223 °C | 433 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® CE15330 NC010 PBT
(Unverified Data**) Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax PBT 1100-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 223 °C | 433 °F | DSC Peak; JIS K7121 |
Goodfellow TPX® DX310 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Melting Point | 223 °C | 433 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® CE15315 BK010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0.. |
|||
Melting Point | 223 °C | 433 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® FGS600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Melting Point | 223 °C | 433 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® SK692FR BK507 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK692FR is a 15% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided by .. |
|||
Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NB40 GR20 NL XA 20 PA 6 20% glass fiber reinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NB40 KK30 NL PA 6 30% glass fiber/mineral reinforced, low warpage Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NB40 NL E PA 6 lubricated, nucleated Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NB40 NL IH PA 6 impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NB40 NL RM PA6, unfilled, MoS2, natural Information provided by Eurotec® |
|||
Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NB40 GR15 NL PA 6 15% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 223 °C | 433 °F | ASTM Test |
BASF Ultradur B 2300 G6 HR BK15116 30% Glass Filled PBT Ultradur B 2300 G6 HR BK15116 is a hydrolysis resistant, pigmented black 30% fiberglass reinforced PBT, exhibiting superior flow characteristics. Designed for improved latch
strength in automotive.. |
|||
Melting Point | 223 °C | 433 °F | 10 K/min |
BASF Ultradur B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET Ultradur B 4040 G10 High Speed BK15029 is a high flow, fast cycling with low warpage, 50% glass filled, injection molding PBT for industrial parts, rigid tough and dimensional stable applications. |
|||
Melting Point | 223 °C | 433 °F | ASTM Test |
BASF Ultradur B 4300 G4 BK5110 20% Glass Filled PBT Ultradur B 4300 G4 BK5110 is an easy flowing, pigmented black, injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Melting Point | 223 °C | 433 °F | ISO 11357-1/-2 |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Melting Point | 223 °C | 433 °F | ISO 11357-1/-2 |
BASF Ultradur® B 4520 High Speed PBT Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF |
|||
Melting Point | 223 °C | 433 °F | 10 K/min |
BASF Ultradur B 4406 G6 BKQ113 7110 30% Glass Filled PBT Ultradur B 4406 G6 BKQ113 7110 is an UL V0 injection molding, pigmented black, PBT grade with 30% glass fiber reinforcement. |
|||
Melting Point | 223 °C | 433 °F | ASTM Test |
BASF Ultradur B 4406 G6 Q113 30% Glass Filled PBT Ultradur B4406 G6 Q113 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement. |
|||
Melting Point | 223 °C | 433 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610
(Unverified Data**) Zytel® RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is a black, unreinforced, toughened and heat stabilised r.. |
|||
Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NB40 GR30 NL IH PA 6 30% glass fiber reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NB40 NL FN70 PA6, unfilled, flame retardant - halogen free (RoHS compliant), natural Information provided by Eurotec® |
|||
Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NB50 BK001 IH PA6, impact modified, black, extrusion grade Information provided by Eurotec® |
|||
Melting Point | 223 °C | 433 °F | HG/T2235 |
Beijing Evergrow Resources MC Nylon Information provided by Beijing Evergrow Resources. |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax PBT 1200-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 223 °C | 433 °F | ISO 11357-1/-2 |
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, .. |
|||
Melting Point | 223 °C | 433 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® S610SF NC010 PBT
(Unverified Data**) Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Informati.. |