Material Notes:
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprietary manufacturing and machining processes to ensure that Arlons properties consistently outperform the competition.Greene, Tweed offers several different Arlon materials, and all provide high tensile strength and elongation properties, excellent shear strength and creep resistance, outstanding fatigue resistance, broad chemical and radiation resistance, and no susceptibility to hydrolysis (steam/hot water). Our engineers work one on one with customers to find the right solution for each specific application.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 124
124
ASTM D785
Hardness, Shore D 91
91
ASTM D2240
Tensile Strength at Break 121 MPa
17500 psi
ASTM D368
Elongation at Break 3.5 %
3.5 %
ASTM D638
Tensile Modulus 8.27 GPa
1200 ksi
ASTM D638
Flexural Strength 197 MPa
28500 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Descriptive Properties Value Comments
Color Gray to Brown