Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exceed™ 1018 FA Blown Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exceed™ 1018 FA Blown Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. These superior strength properties, along with excellent drawability, allow downguaging in bag applications.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ExxonMobil Method
Thickness 25.4 microns
1.00 mil
Melt Flow 1.0 g/10 min
1.0 g/10 min
ASTM D1238
Antiblock Level 4500 ppm
4500 ppm
Slip Level 450 ppm
450 ppm
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 8.96 MPa
1300 psi
at 2% offset; ASTM D882
Film Tensile Strength at Yield, TD 8.27 MPa
1200 psi
at 2% offset; ASTM D882
Film Elongation at Break, MD 470 %
470 %
ASTM D882
Film Elongation at Break, TD 550 %
550 %
ASTM D882
Puncture Energy 1.80 J
1.33 ft-lb
Exxon Mobil Method
Elmendorf Tear Strength, MD 10.6 g/micron
270 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 17.3 g/micron
440 g/mil
ASTM D1922
Dart Drop 22.8 g/micron
580 g/mil
ASTM D1709A
Film Tensile Strength at Break, MD 45.5 MPa
6600 psi
ASTM D882
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
1% Secant Modulus, MD 173 MPa
25100 psi
ASTM D882
1% Secant Modulus, TD 179 MPa
26000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 119 °C
246 °F
Peak Melting Temperature; ExxonMobil Method
Optical Properties Metric English Comments
Haze 16 %
16 %
ASTM D1003
Gloss 42 %
42 %
45°, MD; ASTM D2457
43 %
43 %
45°, TD; ASTM D2457
Descriptive Properties Value Comments
Features PPA and Thermal Stabilizer