Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 22.8 g/micron | 580 g/mil | ASTM D1709A |
ExxonMobil Exceed™ 1018 DA Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Dart Drop | 22.8 g/micron | 580 g/mil | ASTM D1709A |
ExxonMobil Exceed™ 1018 FA Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Dart Drop | 22.8 g/micron | 580 g/mil | 1 mil; ASTM D1709 |
Chevron Phillips K-Resin® KR53 Styrene-Butadiene Copolymer Customer Benefits:Excellent ClarityHigh Surface GlossGood ToughnessGood Heat SealabilityTypical Applications:Medical PackagingProduce PackagingTwist WrapLidstock and Labeling FilmInformation provide.. |
|||
Dart Drop | 22.8 g/micron | 580 g/mil | ASTM D1709A |
ExxonMobil Exceed™ 1018 EA Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Dart Drop | 22.8 g/micron | 580 g/mil | ASTM D1709A |
ExxonMobil Exceed™ 1018 EB Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |