Polymer Property : Antiblock Level = 4500 ppm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Antiblock Level 4500 ppm
4500 ppm
ExxonMobil Exceed™ 1018 DA Blown Film Resin  (discontinued **)
Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. ..
Antiblock Level 4500 ppm
4500 ppm
ExxonMobil Exceed™ 1018 FA Blown Film Resin  (discontinued **)
Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. ..
Antiblock Level 4500 ppm
4500 ppm
ExxonMobil Exceed™ 1012 MJ Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p..
Antiblock Level 4500 ppm
4500 ppm
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..
Antiblock Level 4500 ppm
4500 ppm
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin (Asia Pacific Grade)
Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie..
Antiblock Level 4500 ppm
4500 ppm
ExxonMobil Exceed™ 1023JA Metallocene Polyethylene Resin
Product Description: Exceed 1023JA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1023JA have outstanding tensile, impact strength and puncture. These superior strength propertie..
Antiblock Level 4500 ppm
4500 ppm
ExxonMobil Exceed™ 1018JA Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..
Antiblock Level 4500 ppm
4500 ppm
ExxonMobil LL 3201.22 Premium High Strength Film Resin  (discontinued **)
LL 3201 resins are hexene copolymer LLDPE film resins. Films produced from these resins have excellent tensile, toughness and stiffness properties. These strength properties, along with good drawdow..