Polymer Property : Film Tensile Strength at Break, TD = 31.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
ExxonMobil Exceed™ 1018 DA Blown Film Resin  (discontinued **)
Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. ..
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
ExxonMobil Exceed™ 1018 FA Blown Film Resin  (discontinued **)
Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. ..
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
LyondellBasell Petrothene® GA501020 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent ..
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
LyondellBasell Petrothene® GA501021 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent ..
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
LyondellBasell Petrothene® GA501022 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent ..
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
LyondellBasell Petrothene® GA501023 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent ..
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
ExxonMobil Escorene™ FL 00018 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00018 is a copolymer of ethylene and vinyl acetate. It offers combines toughness, good optical and sealing properties and low gel. In particular, its good behavior in high fr..
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
ExxonMobil Escorene™ UL 00018 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00018 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic..
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
ExxonMobil LDPE LD 317.09 Low Density Polyethylene Resin
Product Description: LD 317.09 resin is a fractional melt index, 6% vinyl acetate copolymer film resin. Film made from LD 317.09 offers excellent impact strength, tensile properties and heat sealabi..
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
ExxonMobil Exceed™ 1018 EA Blown Film Resin  (discontinued **)
Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. ..
Film Tensile Strength at Break, TD 31.7 MPa
4600 psi
ASTM D882
ExxonMobil Exceed™ 1018 EB Blown Film Resin  (discontinued **)
Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. ..