Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nilit FRIANYL B63 SG40 Nylon 6 for injection molding, 40% mineral filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Mineral Filled
Manufacturer Nilit (formerly Frisetta Polymer)
Trade Name FRIANYL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit FRIANYL B63 SG40 Nylon 6 for injection molding, 40% mineral filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Water Absorption 1.5 - 2.5 %
1.5 - 2.5 %
ISO 62
Water Absorption at Saturation 6.0 - 7.0 %
6.0 - 7.0 %
ISO 62
Viscosity Measurement 145
145
Viscosity index; ISO 307
Linear Mold Shrinkage 0.0080 - 0.018 cm/cm
0.0080 - 0.018 in/in
FRISETTA Test Method
Mechanical Properties Metric English Comments
Ball Indentation Hardness 135 MPa
19600 psi
ISO 2039-1
Tensile Strength at Break 60.0 MPa
8700 psi
ISO 527
Elongation at Break 30 %
30 %
ISO 527
Tensile Modulus 3.00 GPa
435 ksi
ISO 527
Flexural Strength 75.0 MPa
10900 psi
ISO 178
Flexural Modulus 2.70 GPa
392 ksi
ISO 178
Charpy Impact Unnotched NB
NB
DIN 53453
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
DIN 53453
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ISO 3146 DSC
Maximum Service Temperature, Air 105 °C
221 °F
Continuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 195 °C
383 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
ISO 75
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 450 V
450 V
CTI 100; IEC 112