Eurotec® Tecomid® NB40 NL E PA 6 lubricated, nucleated

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Eurotec
Trade Name Tecomid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecomid® NB40 NL E PA 6 lubricated, nucleated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good chemical resistanceGood flow and processing propertiesAPPLICATIONS: AutomotiveElectrical/ElectronicFurnitureConstructionHome appliances
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Filler Content 0.00 %
0.00 %
ISO 3451
Moisture Absorption at Equilibrium 3.0 %
3.0 %
Humidity Absorption, 50% RH, 23°C; ISO 62
Water Absorption at Saturation 10 %
10 %
23°C; ISO 62
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
Linear Mold Shrinkage, Transverse 0.012 cm/cm
0.012 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ISO 527
Elongation at Yield 4.0 %
4.0 %
ISO 527
Tensile Modulus 3.00 GPa
435 ksi
ISO 527
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
6.00 kJ/m²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/eU
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eA
0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
10 K/min; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 180 °C
356 °F
ISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75-1/2
Vicat Softening Point 200 °C
392 °F
50N; ISO 306
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
plaque; IEC 60695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Comparative Tracking Index 600 V
600 V
IEC 60112