Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 0.700 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVAMID 6 GF 15 Polyamide 6, 15% Glass Fiber
FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and ..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVAMID 66 GF 30 HTS Polyamide 66, 30% Glass Fiber, Thermal and Hydrolysis Stabilization
FeaturesPA 66 for injection moulding, chemically reinforced with 35% glass fiber, heat stabilized and stabilized against hydrolysis. Used for cooling water systems in the automotive industry. Deli..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB SCANMID 6 B12^ NH9 Nylon 6, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB SCANTEC PC S60R GF10 V0 Polycarbonate, Glass-Fiber Reinforced, Flame Retardant
Information provided by Polykemi AB
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific)
Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Arnite® CCT GF20 (T-X01415) PBT-20% Glass Reinforced (European Grade)  (discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 GF 15 MI/2 PA6, 15% glass fibre, improved strength
FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Arnite® D04 300 PET (European Grade)  (discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® E53 NC010 Nylon 66  (Unverified Data**)
Zytel® E53 NC010 is a very high viscosity polyamide 66 resin for extrusion.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 0.700 J/cm²

@Temperature -20.0 °C
3.33 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 2-3302 TO BU Elastomer Modified, UV-Stabilized Polypropylene Block-Copolymer
INNOPOL® CS 2-3302 TO BU is an elastomer modified, UV-stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3302 TO BU is developed for producing injection molded automotive..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 2-9110 10% Talc-Filled Polypropylene Block-Copolymer
INNOPOL® CS 2-9110 is a 10% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9110 is developed for producing..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal..
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Styrolution Novodur® H950 ABS
Novodur H950 is a very high heat injection molding grade with high gloss surface appearanceInformation provided by Styrolution
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Sax Polymers SAXAMID 126F3 Nylon 6, 15% Glass Fiber
SAXAMID 126F3 is a polyamide 6 injection-molding-grade reinforced with 15% glass fibers.Information provided by SAX Polymers
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Evonik Corporation Vestamid® LX9013 Plasticized Nylon 12
Description: VESTAMID LX9013 is a plasticized polyamide 12 compound with an especially high long-term resistance under thermal load. Parts made of this material absorb only little moisture, thus lea..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Evonik Corporation Vestodur® 3013 High Viscosity, Hydrolysis Resistant PBT
Description: Degussa AG’s High Performance Polymers Business Unit manufactures a range of polybutylene terephthalate compounds that are supplied under the registered trademark VESTODUR® . Material..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Evonik Corporation Vestodur® 3030 High Viscosity, Hydrolysis Resistant PBT
Description: Degussa AG’s High Performance Polymers Business Unit manufactures a range of polybutylene terephthalate compounds that are supplied under the registered trademark VESTODUR® . Material..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Arnite® TV4 240 PBT-20% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eA
Eurotec® Tecodur® PB70 GR15 NL XA 20 PBT 15% glass fiber reinforced, UL94 V0
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Eurotec® Tecomid® NA40 KK30 NL PA 6.6 30% glass fiber/mineral reinforced, low warpage
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Eurotec® Tecomid® NA40 GR15 NL XA 20 PA 6.6 15% glass fiber reinforced, UL94 V0
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® 21SPC Nylon 66, Conditioned
Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering ..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVAMID 6 T 30 Polyamide 6, 30% Micronized Talc
FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin..
Charpy Impact, Notched 0.700 J/cm²

@Thickness 102 mm,
Temperature -20.0 °C
3.33 ft-lb/in²

@Thickness 4.00 in,
Temperature -4.00 °F
ISO 179
Premix Thermoplastics PRE-ELEC® PA 1409 Conductive Thermoplastic Compound
PRE-ELEC® PA 1409 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1..
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Evonik Corporation Vestamid® X7094 Black Nylon 612 (Dry as Molded)
Description: medium-viscosity, heat-stabilizedApplications: profilesInformation provided by degussa.
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Sax Polymers SAXATEC 4210 Acrylonitrile Styrene Acrylate
SAXATEC 4210 is a high heat resistant, high viscosity and weatherable ASA injection molding grade, characterized by high impact strength and high stiffness.Information provided by SAX Polymers
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Crastin® LW9030 BK851 PBT  (Unverified Data**)
Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Sax Polymers SAXATEC 4120 Acrylonitrile Styrene Acrylate
SAXATEC 4120 is a easy lowing, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX Polym..
Copyright © lookpolymers.com All Rights Reserved