| Eurotec® Tecodur® PB50 NL PBT, unfilled, natural, high viscosity |
Polybutylene Terephthalate (PBT), Unreinforced, Molded |
Tecodur®
|
| Eurotec® Tecodur® PB70 BR20 NL100 HS PBT, 20% glass fiber reinforced, heat stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 GF45 NL PBT 45% filled, high gloss, increased density |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR15 BK002 XA21 PBT, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR30 NL CA 01 PBT/PET 30% glass fiber reinforced |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR30 NL XA 20 PBT 30% glass fiber reinforced, UL94 V0 |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR30 NL XA70 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecolen® HP30 NL XA80 PPHP, flame retardant, halogen free, heat stabilized, natural |
Polypropylene, Flame Retardant |
Tecolen®
|
| Eurotec® Tecomid® NA40 GR14 NL MC PA6.6, 14% glass fiber reinforced, impact modified, heat stabilized, natural |
Nylon 66, 10% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR15 GR003 XA70 PA6.6, 15% glass fiber reinforced, flame retardant - halogen free (RoHS compliant), heat stabilized, grey RAL 7035 |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR20 NL HS PA6.6, 20% glass fiber reinforced, heat stabilized, natural |
Nylon 66, Heat Stabilized |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR30 NL PA 6.6 30% glass fiber reinforced |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR30 NL RT PA 6.6 30% glass fiber reinforced, very low friction and wear |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR30 NL RT PA6.6, 30% glass fiber reinforced, PTFE modified, natural |
Nylon 66, PTFE Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 MR15 NL IL PA6.6, 15% mineral filled, impact modified, natural |
Nylon 66, 20% Mineral Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 NL E PA 6.6 lubricated, nucleated |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 NL FA 50 PA 6.6 unreinforced, UL94 V0, halogen/phosphorus free |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 NL RM PA 6.6 low friction and wear |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA43 GR25 NL XA43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, heat stabilized, natural, UL registered |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NB40 GR20 NL XA 20 PA 6 20% glass fiber reinforced, UL94 V0 |
Nylon 6 |
Tecomid®
|
| Eurotec® Tecomid® NB40 GR20 NL XA60 PA6, 20% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NB40 GR30 NL IM PA6, 30% glass fiber reinforced, impact modified, natural |
Nylon 6, 30% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NB40 GR40 NL PA 6 40% glass fiber reinforced |
Nylon 6 |
Tecomid®
|
| Eurotec® Tecomid® NB40 GR45 NL HS PA6, 45% glass fiber reinforced, heat stabilized, natural |
Nylon 6, 30% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NB40 NL IH PA 6 impact modified |
Nylon 6 |
Tecomid®
|
| Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural |
Polyphthalamide (PPA), 30% Glass Fiber Reinforced |
Tecomid®
|
| Eurotec® Tecopet® PT70 GR15 NL100 PS20 PET, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade |
Polyethylene Terephthalate (PET), 20% Glass Reinforced |
Tecopet®
|
| Eurotec® Tecopet® PT70 GR20 NL100 PR PET, 20% glass fiber reinforced, heat stabilized, natural, fast crystallization grade |
Polyethylene Terephthalate (PET), 20% Glass Reinforced |
Tecopet®
|
| Eurotec® Tecodur® PB70 GR15 NL PBT 15% glass fiber reinforced |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR30 NL XA60 PBT, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus, heat stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 KK45 NL XA 20 PBT 45% glass fiber/mineral reinforced, UL94 V0, low warpage |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecoform® PO20 NL RM POM, MoS2 modified, natural |
Acetal (POM) |
Tecoform®
|
| Eurotec® Tecolen® CP20 MF20 NL XA70 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural |
Polypropylene, Flame Retardant |
Tecolen®
|
| Eurotec® Tecolen® CP20 MF20 NL XC30 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural |
Polypropylene, Flame Retardant |
Tecolen®
|
| Eurotec® Tecomid® MB40 GR20 NL PA6, 20% glass fiber reinforced, natural |
Nylon 6, 20% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 NL XA 20 PA 6.6 unreinforced, UL94 V0 |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NB40 GR30 NL HW PA6, 30% glass fiber reinforced, hydrolysis stabilized, natural |
Nylon 6, 30% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade |
Polyethylene Terephthalate (PET), 30% Glass Reinforced |
Tecopet®
|
| Eurotec® Tecopet® PT70 KK45 PET, 45% glass fiber/mineral reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural |
Polyethylene Terephthalate (PET), Glass/Mineral Reinforced |
Tecopet®
|
| Eurotec® Tecotek® BC43 UF65 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, standard grade |
Polycarbonate/ABS Alloy, Unreinforced |
Tecotek®
|
| Eurotec® Tecotek® PC30 NL RX PC, unfilled, improved flow & low temperature impact, natural |
Polycarbonate, Impact Modified |
Tecotek®
|
| Eurotec® Tecotek® PC30 NL VB03 PC, unfilled, UV stabilized, high impact, natural |
Polycarbonate, Impact Modified |
Tecotek®
|
| Eurotec® Tecotek® PC43 GR20 BK002 PC, 20% glass fiber reinforced, black |
Polycarbonate, 20% Glass Filled |
Tecotek®
|
| Eurotec® Tecotek® PC43 GR30 BK002 PC, 30% glass fiber reinforced, black |
Polycarbonate, 30% Glass Filled |
Tecotek®
|
| Eurotec® Tecotek® PC44 GR10 GR003 ZG70 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), light grey |
Polycarbonate, 10% Glass Filled |
Tecotek®
|
| Eurotec® Tecomid® NB40 GR30 NL XA60 PA6, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NB40 GR50 NL PA6, 50% glass fiber reinforced, natural |
Nylon 6, 50% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NB40 NL IH PA6, impact modified, natural |
Nylon 6, Impact Grade |
Tecomid®
|
| Eurotec® Tecomid® NB400 GR15 NL MB PA6, 15% glass fiber reinforced, impact modified, heat stabilized, natural |
Nylon 6, 20% Glass Fiber Filled |
Tecomid®
|