Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ASTM D648 |
Proto3000 Duraform® AF Selective Laser Sintering (SLS®) Prototyping Polymer Description: Polyamide (nylon) material with metallic appearance for real-world physical testing and functional use.Features:Metallic appearance with nice surface finishGood powder recycle character.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANAMID 66 A53^EM Nylon 66, Modified Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANMID 6 B11^ Nylon 6 Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 75/2Bf |
Radici Radilon® CAHS (dry) Copolyamide 66/6 General purposeInformation provided by Radici group. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C @Thickness 3.20 mm |
356 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP COLORCOMP PX99848 PA 6 LNP* COLORCOMP* PX99848 is an unfilled Nylon 6 resin. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Annealed; ISO 75-1/-2 |
DuPont Performance Polymers Crastin® S600F10 BK851 PBT
(Unverified Data**) Crastin® S600F10 BK851 is an unreinforced, lubricated, medium high viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 - 220 °C | 356 - 428 °F | Average value: 210 °C Grade Count:63 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 - 192 °C | 356 - 378 °F | Average value: 185 °C Grade Count:3 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ASTM D648 |
Firestone CLM200-001 Nylon 6 Used for monofiliament extrusion. Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN111 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN131 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | DIN 53461; ASTM D648 |
Kolon Kopa® KN1331 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | |
LATI Lasulf PSU Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | DIN 53461; ASTM D648 |
Kolon Kopa® KN133 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C @Thickness 3.20 mm |
356 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON IS000XXL PA6.12 LNP* STAT-KON* IS000XXL is a compound based on Nylon 6/12 containing Stainless Steel Fibers. Added features of this material include: Food Contact Compliant Raw Materials, Metal Detectable, Electr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C @Thickness 3.20 mm |
356 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Europe-Africa-Middle East) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C @Thickness 3.20 mm |
356 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Asia Pacific) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 75-1/2 |
Suzhou Hipro Polymers Hiprolon® 400 MC HLS G30 Nylon, 30% glass fiber filled Hiprolon® 400 MC HLS G30 is a specialty long chain polyamide compound reinforced with 30% chopped glass fiber for injection molding. It contains some bio-renewable resources Features: high dime.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | dry; ISO 75-1/-2 |
DSM Novamid® 1010C2 PA6 Easy Molding Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® AZ 3 PA66 Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6000 SUVCP Nylon 6, Finely Crystalline, UV Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | annealed; ISO 75-1/-2 |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Eurostar Staramide B28 PA6, Injection Molded Staramide B28 is an Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | |
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 75-1/-2 |
DSM Akulon® F232-DH Nylon 6 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 75 |
BASF Ultramid® B3S BK00464 PA6 (Dry) Ultramid B3S BK00464 is an easy flowing, pigmented black, finely crystalline injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |