Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Engineered Polymer Solutions ABS PCR 400, Recycled

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Engineered Polymer Solutions
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Engineered Polymer Solutions ABS PCR 400, Recycled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Purpose with 40% Post Consumer ABS. Natural and colors available. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792-91
Melt Flow 7.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D638
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 2.45 GPa
355 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 177 - 193 °C
350 - 380 °F
Middle Barrel Temperature 177 - 204 °C
350 - 400 °F
Front Barrel Temperature 193 - 204 °C
380 - 400 °F
Nozzle Temperature 204 - 221 °C
400 - 430 °F
Mold Temperature 48.9 - 60.0 °C
120 - 140 °F
Drying Temperature 79.4 - 85.0 °C
175 - 185 °F
Dry Time 2 - 4 hour
2 - 4 hour