Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE) Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough.. |
|||
Middle Barrel Temperature | 177 - 204 °C | 350 - 400 °F | |
Star Plastics ABS450FR Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 177 - 204 °C | 350 - 400 °F | |
Star Plastics ABSFR1 Molding Grade ABSFR Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3135 can be processed by injection molding or extrusion for ap.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3145D Thermoplastic Elastomer A high hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3145D can be processed by injection blow molding, molding or .. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3480N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3490N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4165 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4165 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4175 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4175 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4180 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4180 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4190 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4190 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Middle Barrel Temperature | 188 - 204 °C | 370 - 400 °F | Extrusion Metering Zone |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
Middle Barrel Temperature | 188 - 204 °C | 370 - 400 °F | Extrusion Metering Zone |
Teknor Apex Sarlink® 4380 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4380 is a flame retardant, medium hardness grade processing exceptional chemical resistance, compression s.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4390 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4390 is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Middle Barrel Temperature | 188 - 204 °C | 370 - 400 °F | Extrusion Metering Zone |
Teknor Apex Sarlink® 4390 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4390 is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4490 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4490 is a medium hardness grade possessing exceptional tensile strength, superior compressio.. |
|||
Middle Barrel Temperature | 191 - 204 °C | 375 - 400 °F | |
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Middle Barrel Temperature | 177 - 204 °C | 350 - 400 °F | |
Engineered Polymer Solutions ABS PCR 400, Recycled General Purpose with 40% Post Consumer ABS. Natural and colors available. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3140 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3140 can be processed by injection molding or extrusion for appl.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3490 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Middle Barrel Temperature | 188 - 204 °C | 370 - 400 °F | Extrusion Metering Zone |
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3150 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3150 can be processed by injection molding or extrusion for appl.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex.. |
|||
Middle Barrel Temperature | 182 - 204 °C | 360 - 400 °F | Extrusion Transition Zone |
Teknor Apex Sarlink® 3439DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |