Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY66-IM2-G33 Nylon 66, 33% Glass Reinforced, Impact Modified Nylon 66, 33% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY66-IM2-G33-[color]-H Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
D 256 |
RTP Company RTP 301 TFE 10 Polycarbonate (PC), Glass Fiber - PTFE Lubricated |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
RTP Company RTP 205D TFE 10 Nylon 6/12 (PA 6/12) Glass Fiber 30% - PTFE 10%
(discontinued Glass Fiber 30% - PTFE 10%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provide.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | 73°F; ASTM D256 |
M. Holland Company AB308LG ABS Acrylonitrile Butadiene Styrene High flowGood impact resistanceHigh stiffnessApplications: Household goodsPackagingInformation provided by M. Holland |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | 73°F; ASTM D256 |
M. Holland Company CP402 Polypropylene Impact Copolymer Impact copolymerGood impact resistanceLow temperature impact resistanceNucleatedGood stiffnessApplications: CratesLawn and garden equipmentTool/tote box |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF30 IM HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature -28.9 °C |
3.50 ft-lb/in @Temperature -20.0 °F |
ASTM D256 |
Spartech Royalite R24 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Chemlon® 233 GI Nylon 6, 33% Glass Fiber Reinforced Features: High Impact, 33% Glass Reinforced; Highly toughened compound exhibiting strength and rigidity; Good Creep Resistance; Good Stiffness; Good Toughness; Impact Modified Processing Method: Inj.. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF30 IM2 UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: UV Stabilizer, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Good UV.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Chemlon® 345G Nylon 610, Glass Fiber Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Westlake Plastics Corzan® II CPVC Sheet Corzan® II CPVC, manufactured from Corzan G2 resin, was developed for use in the construction of wet benches and other cleanroom equipment for the semiconductor industry. It meets Factory Mutual.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Westlake Plastics Norylux™ EN-265 Modified Polyphenylene Oxide Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most d.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
D 256 |
RTP Company PermaStat® 300 FR A Polycarbonate (PC), ESD Protection - Permanently Anti-static - Flame Retardant |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.20 mm |
3.50 ft-lb/in @Thickness 0.126 in |
ASTM D 256 |
RTP Company PermaStat® 600 CLEAR Acrylonitrile Butadiene Styrene (ABS) Permanently Anti-static - ESD Protection - Transparent Grade - No Tint |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Engineered Polymer Solutions ABS 450 Low Gloss, Medium Impact. Natural and colors available. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Engineered Polymer Solutions PPE/PA 9100 PPE/Nylon Alloy. Natural and colors available. Injection molding grade. Uses: General Purpose, paintable, plate-ableInformation provided by Engineered Polymer Solutions. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger NORYL® Polyphenylene oxide (PPO) NORYL®, due to its inherent chemical composition, exhibits unusually low moisture absorption. Therefore, good electrical insulating properties are realized over a wide range of humidity and temper.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256A |
Dow C133-02 Polypropylene Impact Copolymer Resin OverviewDow C133-02 Polypropylene Resin is intended for use in extrusion, thermoforming, and extrusion blow molding applications where impact at refrigeration temperatures is desired. It is especia.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Engineered Polymer Solutions ABS PCR 400, Recycled General Purpose with 40% Post Consumer ABS. Natural and colors available. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
3.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ABS TS-12 Injection Molding Grade, Medium Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Aclo Accuguard Polycarbonate POL050G10HIV0L Glass Reinforced High Impact Flame Retardant |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 257 PPO A high flow grade for applications requiring high impact strength, heat resistance and dimensional stability.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.87 J/cm @Diameter 3.17 mm |
3.50 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 6260 Super High Impact Polystyrene
(discontinued **) Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined.. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
D 256 |
RTP Company RTP 2299 X 108578 A Polyetheretherketone (PEEK), Long Glass Fiber |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
D 256 |
RTP Company VLF 84709 Polytrimethylene Terephthalate (PTT), Long Glass Fiber
(discontinued **) Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
D 256 |
RTP Company RTP 2305 A Rigid Thermoplastic Polyurethane (RTPU), Glass Fiber |