Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.87 J/cm @Temperature 23.0 °C |
3.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT4650-581UV Thermoplastic Polyolefin, UV Stabilized, HD2 Medium Quartz Metallic Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 25-2003 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY66-IM2-G33-[color]-H Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY66-IM-G40 Nylon 66, 40% Glass Reinforced, Impact Modified Nylon 66, 40% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced Superior Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Izod Impact, Notched | 1.87 - 3.20 J/cm | 3.50 - 6.00 ft-lb/in | ASTM D265 |
Alcoa KAMA 3400 Super High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 23.0 °C |
3.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Kleerdex Kydex® 130 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Decorative thermoplastic sheetApplications: Appliances, laminations, electronics, in-store displays, medical devices, equipment housings, dental equipmentFeatures: For deep to hard to form parts or .. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 31% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | 73°F; ASTM D256 |
M. Holland Company CP402 Polypropylene Impact Copolymer Impact copolymerGood impact resistanceLow temperature impact resistanceNucleatedGood stiffnessApplications: CratesLawn and garden equipmentTool/tote box |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 LGCF50 HS BK 6mm 50% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAp.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics ABS450FR Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics ABS5035 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PA6/6,6 GF60 HS L 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat.. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF33 IM HS L BKN 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
PlastxWorld CEVIAN® A2606 30% GF PA/ABS Alloy, Conditioned Property data is for samples at equilibrium moisture (0.7%)These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWo.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® NN133GLUV (COND, 50% RH) Nylon 66, 33% Glass Fiber Reinforced, Internally Lubricated, UV Stabilized Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Westlake Plastics Norylux™ EN-265 Modified Polyphenylene Oxide Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most d.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Westlake Plastics Propylux® CN-P Polypropylene (conductive) Carbon-powder-filled lightweight material with good chemical resistance, extremely low water absorption level, and high impact resistance (no break, notched or unnotched). Rated UL94 V-0.Informatio.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger NORYL® Polyphenylene oxide (PPO) NORYL®, due to its inherent chemical composition, exhibits unusually low moisture absorption. Therefore, good electrical insulating properties are realized over a wide range of humidity and temper.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | molded and tested in accordance with ASTM D 4101; ASTM D256A |
Dow C719-35RNHP Polypropylene Resin DOW C719-35RNHP is intended for use in injection molding applications requiring a good impact/stiffness balance.Information provided by DowDow Announced Sale of Global Polypropylene Business to Bras.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol BR7039 Nylon 6 Alloy, bondable to TPU Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256A |
Braskem TI4040WT Impact Copolymer Polypropylene Description: Superior drop impact at refrigeration temperature, very high flexural modulus, nucleated, good mold release.Applications: Suggested uses include thermoforming, food packaging, dairy con.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene CP0405UVV Copolymer UV Stabilized Approved to Suzuki PP-S2 Med Grey T01 |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 23.0 °C |
3.50 ft-lb/in @Temperature 73.4 °F |
ASTM D-256 |
Axiall 3027 Rigid PVC, Extrusion Georgia Gulf 3027 is a powder blend designed as a substrate base for coextruded profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |