Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Asia Pacific) Reinforced PC/ABS with high stiffness and low CTE. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 101 PC (Asia Pacific) Nonhalogenated, 7.0 MFR, for thicker sections without sinks. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 103R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 104 PC (Asia Pacific) LEXAN 104 is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Melt Flow | 7.0 - 11 g/10 min @Load 5.00 kg, Temperature 200 °C |
7.0 - 11 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
NIZHNEKAMSKNEFTEKHIM 524B General Purpose Polystyrene Polystyrene intended to produce glossy coating by co-extrusion. A specialty recipe provides for drastic reduction of buildup in a die plate and of streaks on an article in molding.Information provi.. |
|||
Melt Flow | 7.0 - 10 g/10 min @Load 2.16 kg, Temperature 230 °C |
7.0 - 10 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 4310M (EP1X30F) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® 5% LF-0718-A in PF-0118-B LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® LUX9612G PC (Asia Pacific) Lexan LUX9612G is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS require.. |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | Condition G |
Ineos Nova 2504 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Good balance of flow, strength and heat resistance, USP Class VI Applications: Consumer electronics, HousewaresExposure to gamma radiation in the 2.02-6.06 megarad range has no .. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Nova 2124 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Appearance comparable to ABS, High gloss at 60°=95; at 20°=90, Significantly reduced stress whitening, custom colors, UL94 HB at 0.62 for all colorsApplications: Injection molding, Toys, Small app.. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Kostat 7440 Conductive ABS Compound KOSTAT 7440 is a conductive thermoplastic compound based on Acrylonitrile Butadiene Styrene and a special carbon black. KOSTAT 7440 is not dependant on atmospheric conditions and is used for ESD in.. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical SH625 ABS, High Impact, High Flow Feature: Extrusion Molding, High Impact, High FlowApplication: Ski Flat, MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Lucobit Lucofin® 1400MN Powder Ethylene Butyl Acrylate Lucofin 1400MN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN Powder is softer and more flexible ethane et.. |
|||
Melt Flow | 7.0 g/10 min @Load 6.60 kg, Temperature 337 °C |
7.0 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 360 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem PW2200 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 343 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 649 °F |
ASTM D1238 |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU) Udel® P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and.. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® NH-0925U ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 7.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 2610 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 7.0 g/10 min @Load 8.70 kg, Temperature 224 °C |
7.0 g/10 min @Load 19.2 lb, Temperature 435 °F |
ASTM D1238 |
Lubrizol Estane® 2103-90AE Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
Cossa Polimeri ESTADIENE 1016 T V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, high thermal resistance, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polim.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Covestro Makrolon® KU 1-1248 Polycarbonate, High Impact Medium viscosity BgVV and FDA - injection molding grade, impact modified, specially for chocolate molds, light colors only.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 230 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers NPP25-0715CF20 20% Conductive Filler Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg |
7.0 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 9.1. |
Dow LDPE 779I Low Density Polyethylene DOW LDPE 779I resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent rigidity. Typical applications include caps.. |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Homopolymer HP0334M40L Mica Reinforced |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Arkema Group Appryl® CZU 0525 Polypropylene, 25% Talc Filled Compound of a PP copolymer modified with EPR and 25% talc. This grade has been specially developed for exterior trim automotive applications, that required an excellent impact test associated with a.. |
|||
Melt Flow | 7.0 - 10 g/10 min @Temperature 230 °C |
7.0 - 10 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min |
Polimeri Europa SINKRAL D720 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-08-35-15 High impact injection moulding grade, with improved flow compared with SINKRAL B620 and a high glo.. |
|||
Melt Flow | 7.0 - 10 g/10 min @Temperature 230 °C |
7.0 - 10 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 2388 Glass Reinforced Polypropylene DescriptionPolyfort® FPP 2388 is a 5% glass reinforced polypropylene.Information provided by A. Schulman. |