Ecomass® 3608TU96 Tungsten Filled Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ecomass Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 3608TU96 Tungsten Filled Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyethylene (HDPE)Information provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 11.0 g/cc
11.0 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 5.78 MPa
839 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Tensile Modulus 2.348 GPa
340.6 ksi
ASTM D638
Flexural Strength 14.2 MPa
2060 psi
ASTM D790
Flexural Modulus 1.97 GPa
286 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.7 °C
170 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.6 °C
150 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.20 ohm
0.20 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 177 - 227 °C
350 - 440 °F
Mold Temperature 21.1 - 65.6 °C
70.0 - 150 °F