Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 286 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.97 GPa
286 ksi
ASTM D790
Omni Plastics OmniLon™ 6 PA6 IM20 Unfilled/ Impact Modified Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Flexural Modulus 1.97 GPa
286 ksi
ASTM D790
Omni Plastics OmniLon™ 6/6 PA6/6 IM20 Unfilled/ Impact Modified Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Flexural Modulus 1.97 GPa
286 ksi
ASTM D790
Ineos Nova FX510 Super High Impact Polystyrene  (discontinued **)
Features: Extremely high impact strengthGood flexural strengthUL Classification 94 HBCustom colors availableApplications: Injection molding or extrusionSuitable replacement for some engineering resi..
Flexural Modulus 1.97 GPa
286 ksi
0.1 in/min; ASTM D790
Ineos Nova 1983 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
Extremely high impact strength with good flexural stiffness, Color Stable, Custom colors, UL94 HB at 0.060 for all colorsApplications: Suitable for extrusion or injection molding processes requiring..
Flexural Modulus 1.97 GPa
286 ksi
ISO 178
Aardvark Polymers AARTEL® 850IM Rotational Molding Resin
Aartel 850 IM is a moderately toughened impact modified acetal copolymer which exhibits ductility in bending and impact loading. The ductile, rather than brittle, failure mode gives designers more f..
Flexural Modulus 1.97 GPa
286 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRILOY D2000 PC
LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Flexural Modulus 1.97 GPa
286 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR
Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries.
Flexural Modulus 1.97 GPa
286 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR
Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries.
Flexural Modulus 1.97 GPa
286 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL HIPS3190 HIPS
Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only.
Flexural Modulus 1.97 GPa
286 ksi
ASTM D790
Ecomass® 3608TU96 Tungsten Filled Polyethylene
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyethylene (HDPE)Information provided by Technical Polymers
Flexural Modulus 1.97 GPa
286 ksi
ASTM Test
BASF Ultraform N 2640 Z2 UNC Q600 POM
Ultraform N2640 Z2 UNC Q600 is an elastomer-modified grade of POM for injection molding with high impact strength.
Flexural Modulus 1.97 GPa
286 ksi
ASTM Test
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Conditioned)
Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the..
Flexural Modulus 1.97 GPa
286 ksi
ASTM D790
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma..
Flexural Modulus 1.97 GPa
286 ksi
ASTM D790
Ineos Nova Zylar® 535 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features: High clarity, strength and toughnessStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationAnti-stat packageEnhanced mold releaseUL 94HB @ 1.5 mm for a..
Copyright © lookpolymers.com All Rights Reserved